We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Gedik · Creep-resisting Cr-Mo steels

OPUS 9 CMV-15 — E9015-B91 H4

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 350 mm
    ≈ 5 kg
  • Ø 3.2 × 350 mm
    ≈ 5 kg
  • Ø 4 × 350 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Do I need to preheat?With this product's data: H5
Thickness of the thickest part in the jointmethod B: d from 10 to 90 mm

100 °C

Minimum preheat and minimum interpass temperature

EN 1011-2, annex C, method B · rounded up to 5 °C

✓ Within the range of method B.

Calculated with: HD 5 ml/100 g from this product's class H5 · 111 — basic electrode: 24 V, 160 A, 15 cm/min

See the full calculation →

Field of application

  • High-alloyed low-hydrogen electrode with basic-type coating
  • Resistance to heat and creep, high resistance to creeping and high toughness values under long-term stress
  • Weld metal’s resistance to high temperatures up to 620°C
  • Pre-heating and inter-pass welding temperature: 200°C - 315°C,
  • Requirement of re-drying for min. 2 hours at the temperatures between 300°C and 350°C

Base metals

X10CrMoVNb 9-1A213 Gr. T91A 335 Gr. P91 (T91)A 139Gr.T91% 9-12 Cr type martensitic stainless steels
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE9015-B91 H4
EN ISO classE CrMo91 B 42 H5

Approvals

  • CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.09
Npresent
V0.20
Cr9.00
Mn0.50
Mo1.00
Nb0.04
Ni1.00
Si0.20
Values in mass %.

Mechanical properties

Service temperaturemax. 620 °C
after heat treatment: 745–775 °C / 2 h / 300 °C (air)
Yield strength (Rp0.2)min. 530 MPa
Tensile strength (Rm)min. 620 MPa
Elongation (A5)min. 17 %
Impact energy (KV)min. 47 J (20 °C)

How to weld

Treatment and preparation

Re-drying300–350 °C / min. 2 h
Pre-heating200–315 °C
Interpass temperature200–315 °C

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–110 A
3.2 mm350 mm110–140 A
4 mm350 mm140–190 A
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassAvailability
OPUS 9 CMVGedikE CrMo91 B 42 H5To order · price and lead time in the quote