Gedik · Creep-resisting Cr-Mo steels
OPUS 9 CMV — E9018-B91 H4
covered electrode · stick electrodebasic coating
Choose the size
- Ø 2.5 × 350 mm≈ 5 kg
- Ø 3.2 × 350 mm≈ 5 kg
- Ø 4 × 350 mm≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
Do I need to preheat?With this product's data: H5
Thickness of the thickest part in the jointmethod B: d from 10 to 90 mm
100 °C
Minimum preheat and minimum interpass temperature
EN 1011-2, annex C, method B · rounded up to 5 °C
✓ Within the range of method B.
Calculated with: HD 5 ml/100 g from this product's class H5 · 111 — basic electrode: 24 V, 160 A, 15 cm/min
See the full calculation →Field of application
- High-alloyed low-hydrogen electrode with basic-type coating
- Resistance to heat and creep, high resistance to creeping and high toughness values under long-term stress
- Weld metal’s resistance to high temperatures up to 620°C
- Pre-heating and inter-pass welding temperature: 200°C - 315°C
- Requirement of re-drying for min. 2 hours at the temperatures between 300°C and 350°C
Base metals
X10CrMoVNb 9-1A213 Gr. T91A 335 Gr. P91 (T91)A 139Gr.T91% 9-12 Cr type martensitic stainless steels
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up |
|---|---|
| Polarity | DC+ |
Classification and approvals
Classification
| AWS class | E9018-B91 H4 |
|---|---|
| EN ISO class | E CrMo91 B 42 H5 |
Approvals
- CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.09 |
|---|---|
| N | present |
| V | 0.20 |
| Cr | 9.00 |
| Mn | 0.50 |
| Mo | 1.00 |
| Nb | 0.04 |
| Ni | 0.60 |
| Si | 0.20 |
Values in mass %.
Mechanical properties
| Service temperature | max. 620 °C |
|---|
after heat treatment: 745–775 °C / 2 h / 300 °C (air)
| Yield strength (Rp0.2) | min. 530 MPa |
|---|---|
| Tensile strength (Rm) | min. 620 MPa |
| Elongation (A5) | 17 % |
| Impact energy (KV) | min. 47 J (20 °C) |
How to weld
Treatment and preparation
| Re-drying | 300–350 °C / min. 2 h |
|---|---|
| Pre-heating | 200–315 °C |
| Interpass temperature | 200–315 °C |
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 350 mm | 80–110 A |
| 3.2 mm | 350 mm | 110–140 A |
| 4 mm | 350 mm | 140–190 A |
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same EN ISO designation
| Product | Class | Availability |
|---|---|---|
| OPUS 9 CMV-15Gedik | E CrMo91 B 42 H5 | To order · price and lead time in the quote |