We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Nickel alloys

FINOX 625 — E NiCrMo-3

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2.5 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Which filler joins two different metals?With this product's data: Ni 6625

Suitable

The Schaeffler diagram does not apply to a nickel-base weld; the service assessment is shown.

✓

Calculated with: filler Ni 6625 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Nickel-base electrode for joining and cladding on matching nickel-chromium-molybdenum steels and similar nickel-chromium steels, (heat-resisting) Cr and CrNi (Mo, N) steels and nickel-alloyed pressure vessel steels tough at low temperatures. Use at service temperatures from -196 °C up to 1,000 °C (in sulphur-containing atmospheres only up to 500 °C). The fully austenitic weld metal is corrosion-resisting, tough at low temperatures, with high-temperature strength, resistant to scaling up to 1,000 °C and not susceptible to embrittlement. High resistance to corrosive media.

Base metals

1.4529 X 1 NiCrMoCuN 25-20-71.4876 X 10 NiCrAlTi 32-212.4816 NiCr 15 Fe2.4856 NiCr 22 Mo 9 Nb2.4858 NiCr 21 MoAlloy 600Alloy 625Alloy 800Alloy 825
PositionsPA flat PB horizontal-vertical PC horizontal PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS classE NiCrMo-3
EN ISO classE Ni 6625 (NiCr22Mo9Nb)
Material no. (W.-Nr.)2.4621

Composition and properties

Chemical composition of the weld metal

C0.04
Cr22.0
Mn0.20
Mo9.00
Nb3.50
Nibalance
Si0.25
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 420 MPa
Tensile strength (Rm)> 760 MPa
Elongation (A5)> 30 %
Impact energy (KV)> 90 J (room temperature) · > 40 J (−196 °C)

How to weld

Treatment and preparation

Re-drying250–300 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm90–120 A
3.25 mm350 mm120–160 A
4 mm350 mm150–190 A
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassRmKVAvailability
NIBAZ B 65GedikE Ni 6625 (NiCr22Mo9Nb)min. 760 MPamin. 60 J (20 °C)To order · price and lead time in the quote