We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Gedik · Nickel alloys

NIBAZ B 65 — E NiCrMo-3

covered electrode · stick electrode

Choose the size

  • Ø 2.5 × 250 mm
    ≈ 5 kg
  • Ø 3.2 × 300 mm
    ≈ 5 kg
  • Ø 4 × 350 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Which filler joins two different metals?With this product's data: Ni 6625

Suitable

The Schaeffler diagram does not apply to a nickel-base weld; the service assessment is shown.

✓

Calculated with: filler Ni 6625 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

  • High Molybdenum Nickel-base alloy electrode for creep-resistant steels, heat resisting steels, heat resisting and Cryogenic materials, dissimilar joints and high strength problem steels
  • Especially designed for Inconel 625 and Incoloy 825
  • Re-drying cond.: 250°C-300°C / 2h

Base metals

1.4529 X2 NiCrMoCu 25 20 61.4583 X10 NiCrMoNb 18121.4876 X10 NiCrAlTi 32 20 (incoloy800)1.5662 X8 Ni 9 (ASTM 9Ni)2.4816 NiCr 15 Fe (inconel 600)2.4856 NiCr 22 Mo 9 Nb (inconel 625)2.4858 NiCr 21 Mo (inconel 825)2.4951 NiCr20Ti (ASTM 75)2.4952 NiCr 20 TLN (ASTM 80A)
ASTM:
844384448446 (UNS N06625)
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE NiCrMo-3
EN ISO classE Ni 6625 (NiCr22Mo9Nb)

Approvals

  • SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.04
Cr21.0
Fe5.00
Mn0.40
Mo9.00
Nb3.50
Nibalance
Si0.70
Tipresent
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)min. 420 MPa
Tensile strength (Rm)min. 760 MPa
Elongation (A5)min. 30 %
Impact energy (KV)min. 60 J (20 °C) · min. 35 J (−196 °C)

How to weld

Treatment and preparation

Re-drying250–300 °C / 2 h

Welding parameters by diameter

ØLengthCurrent
2.5 mm250 mm60–80 A
3.2 mm300 mm70–100 A
4 mm350 mm90–130 A
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassRmKVAvailability
FINOX 625KjellbergE Ni 6625 (NiCr22Mo9Nb)> 760 MPa> 90 J (room temperature)To order · price and lead time in the quote