Calculators
Dissimilar metal joints — Schaeffler and WRC-1992 diagrams
Where the weld lands given the two base metals, the filler and the dilution: diagram zone, ferrite and ferrite number FN. Use it to choose the filler for carbon steel to stainless or between two different stainless steels.
How we calculate it
- Schaeffler equivalents — Schaeffler 1949Cr eq = Cr + Mo + 1.5·Si + 0.5·Nb Ni eq = Ni + 30·C + 0.5·Mn S355J2: 0.83 / 6.80 · 1.4301: 20.00 / 12.35
- WRC-1992 equivalents — Kotecki & Siewert, 1992Cr eq = Cr + Mo + 0.7·Nb Ni eq = Ni + 35·C + 20·N + 0.25·Cu
ResultSuitable
—
The Schaeffler diagram does not apply to a nickel-base weld; the service assessment is shown.
✓
Fillers for this pair
Butt joint without a buffer layer. Maximum dilution: the highest at which the weld is still acceptable by its structure.
| Filler | Assessment | Max. dilution, % | |
|---|---|---|---|
| 309LMo · E 23 12 2 L | Suitable | 41.5 | |
| 312 · E 29 9 | Suitable | 57.5 | |
| AWS E307 | Suitable | 45.5 | |
| 309L · E 23 12 L | With reservations | 25.5 |
Schaeffler diagramSchaeffler 1949 · Kotecki & Siewert 1992
- metal 1
- metal 2
WRC-1992 — ferrite numberISO 8249 · FN
From the catalogue, for this result
Class ENiCrMo-3 · E Ni 6625, for the chosen process
- See product →NIBAZ B 65AWS ENiCrMo-3 · EN ISO E Ni 6625 (NiCr22Mo9Nb)
- See product →FINOX 625AWS ENiCrMo-3 · EN ISO E Ni 6625 (NiCr22Mo9Nb)
Standards and sources
- Schaeffler, Metal Progress 56 (1949) — constitution diagram: zones A, M and F
- Kotecki & Siewert, Welding Journal 71 (5), 1992 — WRC-1992; lines digitised from its figures 1 and 3
- ISO 8249:2018 — ferrite number FN
- EN ISO 3581:2016 · AWS A5.4 — stainless filler classes
- EN 10025-2:2019 · EN 10088-2:2014 — nominal composition of the base metals
Indicative results: good for planning and ordering material; they do not replace the WPS.