FERVEO INX 310 B

covered electrode · stick electrodeCatalogue only
also as: covered electrode · stick electrodesolid wireTIG rod
AWS class
~E 310-15
EN ISO class
E 25 20 B 22
Tensile strength (Rm)
560–690 MPa

Classification

AWS class~E 310-15
EN ISO classE 25 20 B 22

Purpose

  • Basic-coated variant of INX 310, same Cr-Ni 25/20.5 — wider service range (-196°C to +1200°C) and more toughness than the rutile variant (100 J vs 47 J).

Why it works

Same core as INX 310 R, basic-coated: the manufacturer's impact test gives more than double the toughness (100 J vs 47 J), and the stated service range spans from cryogenic (-196°C) up to +1200°C — the choice when toughness matters alongside hot service.

Fields of application

  • Austenitic Cr-Ni steels, ferritic Cr-Ni-Al steels, heat-resistant cast/forged/rolled steels.
  • Ceramics, petrochemical industry, furnaces, boilers, chimneys.

Chemical composition

ElementTypical, %
C0.12
Cr25
Mn3
Ni20.5
Si0.9

Mechanical properties

Tensile strength (Rm)560–690 MPa
Yield strength (Rp0.2)355 MPa
Elongation (A5)25 %
Impact energy (KV)100 J (20 °C)

Process

PolarityDC+
PositionsPAflatPBhorizontal-verticalPChorizontalPDhorizontal-overheadPEoverheadPFvertical-up

Sizes and part numbers

ØLengthCurrentRequest
2.5 mm250 mm50–80 A
3.2 mm300 mm80–110 A
3.2 mm350 mm80–110 A
4 mm350 mm110–140 A

Cross-reference

Replaces EutecTrode 310-17 (Castolin)Direct replacement
Replaces EutecTrode 310-16 (Castolin)Direct replacement
Replaces EI 310B (Magmaweld)Direct replacement
Replaces NIC 310 (Nicrotec)Direct replacement
Replaces BASINOX 310 (Oerlikon)Direct replacement

Equivalence refers to the classification (AWS / EN ISO), not to product identity. In applications with a qualified procedure (WPS), validate the substitution before use.

Base metals

X15CrNiSi 25 20X12CrNi 25 21X15CrNiSi 20 12G-X 15CrNi 25 20G-X 40CrNi 25 21G-X40CrNiSi22 9X10CrAI 18X10CrAI 24G-X40CrSi 17AISI 305310314.

Advantages

  • Service range -196°C to +1200°C.
  • Higher toughness than the rutile variant (100 J vs 47 J).

Limitations

Notes