Kjellberg · Creep-resisting Cr-Mo steels
CROMO 1B — E 8018-B2
covered electrode · stick electrodebasic coating
Choose the size
- Ø 2.5 × 350 mm · 4.3 kg≈ 4.3 kg
- Ø 3.25 × 350 mm · 4.8 kg≈ 4.8 kg
- Ø 4 × 350 mm · 4.8 kg≈ 4.8 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
6.97–11.14 kg
of CROMO 1B for 10 m of weld
3 packs of 4.3 kg
Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Field of application
Covered electrode for joining boiler and tube steels and similar CrMo-alloyed steels resistant to hydrogen under pressure, preferably for steel 13CrMo4-5 at service temperatures up to 550 °C. Also suitable for joining and surfacing on similarly alloyed case-hardening and quenched and tempered steels.
Base metals
1.7218 25 CrMo 41.7218 G 25 CrMo 41.7254 20 CrMo 41.7258 24 CrMo51.7262 15 CrMo 51.7335 13 CrMo 4-51.7337 16 CrMo 4-41.7350 22 CrMo 4-41.7354 G22 CrMo 5-4
| Positions | PA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up |
|---|---|
| Polarity | DC+ |
Classification and approvals
Classification
| AWS class | E 8018-B2 |
|---|---|
| EN ISO class | E CrMo1 B 42 |
Approvals
- TÜV, CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.08 |
|---|---|
| Cr | 1.00 |
| Mn | 1.00 |
| Mo | 0.50 |
| Si | 0.40 |
Values in mass %.
Mechanical properties
after tempering: min. 0.5 h at 700 °C, cooling in still air
| Yield strength (Rp0.2) | > 400 MPa |
|---|---|
| Tensile strength (Rm) | 510–650 MPa |
| Elongation (A5) | > 20 % |
| Impact energy (KV) | > 80 J (20 °C) |
How to weld
Treatment and preparation
| Re-drying | 300–350 °C / 2 h |
|---|
Storage
In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.
| Moisture in the covering | More spatter and porosity: redry, above all when low hydrogen content is required. |
|---|
According to the Kjellberg 2019 catalogue
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 350 mm | 90–110 A |
| 3.25 mm | 350 mm | 110–150 A |
| 4 mm | 350 mm | 140–180 A |
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same EN ISO designation
| Product | Class | Availability |
|---|---|---|
| OPUS CMGedik | E CrMo1 B 42 H5 | To order · price and lead time in the quote |
| OPUS CM-15Gedik | E CrMo1 B 42 H5 | To order · price and lead time in the quote |