Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Carbon steels

TITAN ROT — E 6013

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2.5 × 350 mm · 4.8 kg
    ≈ 4.8 kg
  • Ø 3.25 × 350 mm · 4.8 kg
    ≈ 4.8 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.97–11.14 kg

of TITAN ROT for 10 m of weld

3 packs of 4.8 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

Covered electrode for versatile use in industry and workshops. Excellent arc striking, soft arc, little spatter, finely rippled and smooth bead appearance, flat to slightly concave fillet welds, slag generally self-releasing.

Base metals

Non-alloy structural steels: S235 to S355Shipbuilding steels: A, B, D, A32/36, D32/36Pressure vessel steels: P195 to P275Pipeline steels: L210 to L245Cast steels: GE200, GE240, GP240, G20Mo5Reinforcing steels: BSt 420
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC−/AC

Classification and approvals

Classification

AWS classE 6013
EN ISO classE 35 0 RR 12

Approvals

  • DB, TÜV, CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.08
Mn0.40
Si0.25
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 360 MPa
Tensile strength (Rm)450–550 MPa
Elongation (A5)> 22 %
Impact energy (KV)> 55 J (0 °C)

How to weld

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
Re-dryingIf required: 70–100 °C, 60 min.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–100 A
3.25 mm350 mm100–130 A
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same AWS designation
ProductClassRmKVAvailability
EGEGedikE6013470–550 MPamin. 47 J (0 °C)To order · price and lead time in the quote
ELITGedikE6013510–610 MPamin. 47 J (0 °C)To order · price and lead time in the quote
INTERGedikE6013470–590 MPamin. 47 J (0 °C)To order · price and lead time in the quote
LOTUSGedikE6013510–610 MPamin. 47 J (0 °C)To order · price and lead time in the quote
OPTIMALKjellbergE6013510–560 MPa> 60 J (0 °C)To order · price and lead time in the quote
Show all (11)
Same class
same AWS designation
ProductClassRmKVAvailability
PANTERAGedikE6013510–610 MPamin. 47 J (0 °C)To order · price and lead time in the quote
PRIMAKjellbergE6013510–560 MPa> 60 J (0 °C)To order · price and lead time in the quote
PRIMA BLUEKjellbergE6013520–600 MPa> 70 J (−10 °C)To order · price and lead time in the quote
TITANKjellbergE6013470–530 MPa> 60 J (20 °C)To order · price and lead time in the quote