Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Carbon steels

TITAN — E 6013

covered electrode · stick electroderutile-basic coating

Choose the size

  • Ø 2.5 × 350 mm · 4.8 kg
    ≈ 4.8 kg
  • Ø 3.25 × 350 mm · 4.8 kg
    ≈ 4.8 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.97–11.14 kg

of TITAN for 10 m of weld

3 packs of 4.8 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

General-purpose electrode, particularly suitable for root and positional welding in pipeline construction, vessel and boiler construction and shipbuilding. Finely rippled, well-formed X-ray quality welds with a smooth transition to the parent metal without undercut. Very easy slag removal, also in root runs.

Base metals

Non-alloy structural steels: S235 to S355Fine-grain structural steels: S275 to S355Shipbuilding steels: A, B, D, E, A32/36, D32/36, E 32/36Pressure vessel steels: P195 to P275Pipeline steels: L210 to L245Cast steels: GE200, GE240, GP240, G20Mo5, G21Mn5Reinforcing steels: BSt 420, BSt 500
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC−/AC

Classification and approvals

Classification

AWS classE 6013
EN ISO classE 38 2 RB 12

Approvals

  • DB, TÜV, CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.08
Mn0.50
Si0.15
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 400 MPa
Tensile strength (Rm)470–530 MPa
Elongation (A5)> 22 %
Impact energy (KV)> 60 J (20 °C)

How to weld

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
Re-dryingIf required: 70–100 °C, 60 min.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–110 A
3.25 mm350 mm110–140 A
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same AWS designation · same EN ISO designation
ProductClassRmKVAvailability
EGEGedikE6013470–550 MPamin. 47 J (0 °C)To order · price and lead time in the quote
ELITGedikE6013510–610 MPamin. 47 J (0 °C)To order · price and lead time in the quote
GRANITGedikE 38 2 RB 12470–570 MPamin. 47 J (−20 °C)To order · price and lead time in the quote
INTERGedikE6013470–590 MPamin. 47 J (0 °C)To order · price and lead time in the quote
LOTUSGedikE6013510–610 MPamin. 47 J (0 °C)To order · price and lead time in the quote
Show all (12)
Same class
same AWS designation
ProductClassRmKVAvailability
OPTIMALKjellbergE6013510–560 MPa> 60 J (0 °C)To order · price and lead time in the quote
PANTERAGedikE6013510–610 MPamin. 47 J (0 °C)To order · price and lead time in the quote
PRIMAKjellbergE6013510–560 MPa> 60 J (0 °C)To order · price and lead time in the quote
PRIMA BLUEKjellbergE6013520–600 MPa> 70 J (−10 °C)To order · price and lead time in the quote
TITAN KKjellbergE6013540–610 MPa> 60 J (−30 °C)To order · price and lead time in the quote
TITAN ROTKjellbergE6013450–550 MPa> 55 J (0 °C)To order · price and lead time in the quote
TITAN SKjellbergE6013510–610 MPa> 60 J (0 °C)To order · price and lead time in the quote