Gedik · Creep-resisting Cr-Mo steels
SG Mo TIG — ER 80 S-G (mod.) (ER 70 S-A1)
TIG rod
also as: solid wire
Choose the size
- Ø 1.6 × 1000 mm · 5 kg≈ 5 kg
- Ø 2 × 1000 mm · 5 kg≈ 5 kg
- Ø 2.4 × 1000 mm · 5 kg≈ 5 kg
- Ø 3.2 × 1000 mm · 5 kg≈ 5 kg
- Ø 4 × 1000 mm · 5 kg≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 141 · η 0.94
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
4.82–6.52 kg
of SG Mo TIG for 10 m of weld
2 packs of 5 kg
Calculated with: η 0.9405: TIG with filler rod, 0.99 less the stub s of a 1000 mm rod · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Field of application
- Copper coated wire for GMAW and rod TIG welding in boiler pressure vessel, pipework and crane construction as well as in structural steel engineering
- High quality, very tough deposit of high crack resistance and non-aging
- Recommended for service in temperature range (-40°C) for TIG, or (-20°C) for GMAW to (+550°C)
- Good copper bonding with low total copper content. Very good welding and flow characteristics
- Preheating interpass and postweld heat treatment as required by base metal
- Shielding gases: MAG; Ar+CO2, mix gases, TIG; %100 Ar
Base metals
S355J2G3L320-L415NBL320MB-L415MBP255G1THP235GH-P355GHP255NH16Mo317MnMoV6-420MnMoNi5-520MnMoNi4-5GE240-GE30022Mo4S255N-S460NP255NH-P460 NH
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up PG vertical-down |
|---|---|
| Polarity | DC− |
| Shielding gas | 100% Ar |
Classification and approvals
Classification
| AWS class | ER 80 S-G (mod.) (ER 70 S-A1) |
|---|---|
| EN ISO class | W MoSi |
Approvals
- CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the wire
| C | 0.10 |
|---|---|
| Mn | 1.10 |
| Mo | 0.50 |
| Si | 0.60 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | min. 460 MPa |
|---|---|
| Tensile strength (Rm) | 550–670 MPa |
| Elongation (A5) | min. 22 % |
| Impact energy (KV) | min. 47 J (−20 °C) |
How to weld
Process
| Shielding | Requires shielding gas |
|---|
Treatment and preparation
| Pre-heating | as required by the base metal |
|---|---|
| Interpass temperature | as required by the base metal |
| Post-weld heat treatment | as required by the base metal |
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same EN ISO designation
| Product | Class | Rm | KV | Availability |
|---|---|---|---|---|
| DT-SG Mo TIGDratec | W MoSi | 560–650 MPa | > 80 J | To order · price and lead time in the quote |