Gedik · Creep-resisting Cr-Mo steels

OPUS P92 — E 9018-B92 (mod.)

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 3.2 × 350 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Field of application

  • Recommended for welding of heat resistant steels T/P92 which are used for steam tubing, turbine casings and power generating casts
  • Provides creep strength and toughness at elevated temperatures with additional alloying elements
  • Weld metal is resistant to temperatures up to +650°C
  • Bruscato factor of X<15
  • Preheat and interpass temperature 200°C-315°C
  • Requirement of re-drying for min. 2 hours at the temperatures between 300°C and 350°C

Base metals

T/P929%Cr1.7%W0.5%Mocreep resisting martensitic steels
ASTM:
A213 Gr T92A 335 Gr P92A387 Gr 92
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE 9018-B92 (mod.)

Approvals

  • SEPRO, CE
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.08
V0.20
W1.80
Cr8.50
Mn0.65
Mo0.50
Ni0.75
Si0.25
Values in mass %.

Mechanical properties

after heat treatment: 745–775 °C / 4 h / 300 °C (air)
Yield strength (Rp0.2)min. 550 MPa
Tensile strength (Rm)min. 650 MPa
Elongation (A5)min. 19 %
Impact energy (KV)min. 47 J (20 °C)

How to weld

Treatment and preparation

Re-drying300–350 °C / min. 2 h
Pre-heating200–315 °C
Interpass temperature200–315 °C

Welding parameters by diameter

ØLengthCurrent
3.2 mm350 mm110–140 A
FERVEO guidance
By problem