Type
covered electrode · stick electrode
Standard
E 9018-B92 (mod.)
Diameters
Ø 3.2 mm
Application
- Recommended for welding of heat resistant steels T/P92 which are used for steam tubing, turbine casings and power generating casts
- Provides creep strength and toughness at elevated temperatures with additional alloying elements
- Weld metal is resistant to temperatures up to +650°C
- Bruscato factor of X<15
- Preheat and interpass temperature 200°C-315°C
- Requirement of re-drying for min. 2 hours at the temperatures between 300°C and 350°C
Classification
AWS class
E 9018-B92 (mod.)
Approvals
SEPRO, CE
Validity is confirmed with the order
Chemical composition of the weld metal
C
V
W
Cr
Mn
Mo
Ni
Si
0.08
0.20
1.80
8.50
0.65
0.50
0.75
0.25
Values in mass %.
Base metals
T/P92 · 9%Cr · 1.7%W · 0.5%Mo · creep resisting martensitic steels
ASTM: A213 Gr T92 · A 335 Gr P92 · A387 Gr 92
Mechanical properties
after heat treatment: 745–775 °C / 4 h / 300 °C (air)
Yield strength (Rp0.2)
min. 550 MPa
Tensile strength (Rm)
min. 650 MPa
Elongation (A5)
min. 19 %
Impact energy (KV)
min. 47 J (20 °C)
Process
Polarity
DC+
Positions
PA flat · PB horizontal-vertical · PC horizontal · PD horizontal-overhead · PE overhead · PF vertical-up
FERVEO IBERICA, S.L.U. · NIF B05613559 · Avda. del Tomillar, 70, 29631 Benalmádena (Málaga) · Registered in the Registro Mercantil de Málaga, sheet MA-201214 · info@ferveo.eu · www.ferveo.eu · FT-OPUS-P92-EN · rev. 2 · page 1 / 2
Typical values, not guaranteed: this document is not a declaration of performance and does not replace the manufacturer's official documentation or the applicable WPS.
Prepared by FERVEO from the Gedik 2023 catalogue