We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Gedik · Creep-resisting Cr-Mo steels

OPUS 2 CML — E 8018-B3 L H4

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 350 mm
    ≈ 5 kg
  • Ø 3.2 × 350 mm
    ≈ 5 kg
  • Ø 4 × 450 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.97–11.14 kg

of OPUS 2 CML for 10 m of weld

3 packs of ≈ 5 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Do I need to preheat?With this product's data: H5
Thickness of the thickest part in the jointmethod B: d from 10 to 90 mm

100 °C

Minimum preheat and minimum interpass temperature

EN 1011-2, annex C, method B · rounded up to 5 °C

✓ Within the range of method B.

Calculated with: HD 5 ml/100 g from this product's class H5 · 111 — basic electrode: 24 V, 160 A, 15 cm/min

See the full calculation →

Field of application

  • Applicability in welding of heat-resisting steels containing 2% Cr - 1% Mn and similar alloys
  • Electrode with basic-type coating
  • Formation of more ductile and less hard weld metal due to low carbon content
  • Serviceability at temperatures of values up to 600 °C
  • Recommended pre-heating and post-heat treatment during welding processes
  • Requirement of re-drying for min. 2 hours at the temperatures between 300°C and 350°C

Base metals

2% Cr-1% Mo SteelsA335 Gr. P22
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE 8018-B3 L H4
EN ISO classE CrMo2L B 42 H5

Approvals

  • CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.04
Cr2.20
Mn0.60
Mo1.10
Si0.60
Values in mass %.

Mechanical properties

Service temperaturemax. 600 °C
after heat treatment: 690–750 °C / 1 h / 300 °C (air)
Yield strength (Rp0.2)min. 530 MPa
Tensile strength (Rm)min. 620 MPa
Elongation (A5)min. 18 %
Impact energy (KV)min. 47 J (20 °C)

How to weld

Treatment and preparation

Re-drying300–350 °C / min. 2 h
Pre-heatingrecommended
Post-weld heat treatmentrecommended

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–110 A
3.2 mm350 mm100–140 A
4 mm450 mm130–180 A
FERVEO guidance
By problem