Basket
Gedik · Carbon steels

LASER B 55 — E 7018 - 1 H4

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 350 mm
    ≈ 5 kg
  • Ø 3.2 × 350 mm
    ≈ 5 kg
  • Ø 4 × 450 mm
    ≈ 5 kg
  • Ø 5 × 450 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.97–11.14 kg

of LASER B 55 for 10 m of weld

3 packs of ≈ 5 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Do I need to preheat?With this product's data: H5
Thickness of the thickest part in the jointmethod B: d from 10 to 90 mm

100 °C

Minimum preheat and minimum interpass temperature

EN 1011-2, annex C, method B · rounded up to 5 °C

✓ Within the range of method B.

Calculated with: HD 5 ml/100 g from this product's class H5 · 111 — basic electrode: 24 V, 160 A, 15 cm/min

See the full calculation →

Field of application

  • Welding of high-strength fine-grain steels and of parts for service at low temperatures down to -50 °C
  • Before use, redry the electrodes at 300-350 °C for 2 h

Base metals

S235JR-E295E335S235J2G3-S355J2G3P235T1-P355T1P235T2P355T2L210NB-L415NBL290MB-L360MBP235G1THP255G1THP235GH-P355GHS235JRS1-S235J4SS315G1 S-S355G3SS255N-S380NP255NH-P355NHS255NL-S460NL1GE200-GE300
API 5L:
X42X46X52X56X60X65
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE 7018 - 1 H4
EN ISO classE 46 5 B 42 H5

Approvals

  • TSE, CE, ABS, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.08
Mn1.40
Si0.40
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)min. 460 MPa
Tensile strength (Rm)530–650 MPa
Elongation (A5)min. 24 %
Impact energy (KV)min. 47 J (−50 °C)

How to weld

Treatment and preparation

Re-drying300–350 °C / min. 2 h

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–100 A
3.2 mm350 mm100–140 A
4 mm450 mm130–190 A
5 mm450 mm190–240 A
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same AWS designation
ProductClassRmKVAvailability
GARANT KKjellbergE7018-1570–620 MPa> 100 J (−40 °C)To order · price and lead time in the quote
GARANT SKjellbergE7018-1540–600 MPa> 90 J (−40 °C)To order · price and lead time in the quote
GARANT XKjellbergE7018-1550–600 MPa> 70 J (−20 °C)To order · price and lead time in the quote
LASER B 50GedikE7018-1 H4510–630 MPamin. 47 J (−50 °C)To order · price and lead time in the quote
LASER B 55-SGedikE7018-1 H4530–650 MPamin. 47 J (−60 °C)To order · price and lead time in the quote