GARANT K — E 7018-1
Choose the size
- Ø 2.5 × 350 mm · 4.6 kg≈ 4.6 kg
- Ø 3.25 × 350 mm · 4.5 kg≈ 4.5 kg
- Ø 3.25 × 450 mm · 6 kg≈ 6 kg
- Ø 4 × 350 mm · 4.8 kg≈ 4.8 kg
- Ø 4 × 450 mm · 6 kg≈ 6 kg
- Ø 5 × 450 mm · 6 kg≈ 6 kg
- Ø 6 × 450 mm · 6 kg≈ 6 kg
We reply within 1 working day.
How much filler metal do I need?With this product's data: 111 · η 0.59
7.68–10.38 kg
of GARANT K for 10 m of weld
Calculated with: η 0.59 — from the datasheet (recovery 120 %, Ø 2.5 × 350 mm) · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Do I need to preheat?With this product's data: H5
100 °C
Minimum preheat and minimum interpass temperature
EN 1011-2, annex C, method B · rounded up to 5 °C
✓ Within the range of method B.
Calculated with: HD 5 ml/100 g from this product's class H5 · 111 — basic electrode: 24 V, 160 A, 15 cm/min
See the full calculation →Field of application
Covered electrode for particularly crack-resistant joining of steels with higher C content, for fine-grain steels tough at low temperatures down to -60 °C. Suitable for offshore applications. Special low-moisture-absorption covering (LMA type).
Base metals
| Positions | PA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up |
|---|---|
| Polarity | DC+ |
Classification and approvals
Classification
| AWS class | E 7018-1 |
|---|---|
| EN ISO class | E 46 4 Z B 42 H5 |
Approvals
- BV, DNV-GL, LR, DB, TÜV, CE, ABS, PRS
Composition and properties
Chemical composition of the weld metal
| C | 0.07 |
|---|---|
| Mn | 1.35 |
| Ni | 0.50 |
| Si | 0.45 |
Mechanical properties
| Yield strength (Rp0.2) | > 490 MPa |
|---|---|
| Tensile strength (Rm) | 570–620 MPa |
| Elongation (A5) | > 24 % |
| Impact energy (KV) | > 100 J (−40 °C) |
How to weld
Process
| Recovery | 120 % |
|---|
Treatment and preparation
| Re-drying | 300–350 °C / 2 h |
|---|
Storage
In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.
| Moisture in the covering | More spatter and porosity: redry, above all when low hydrogen content is required. |
|---|---|
| LMA covering | Redrying only every 8 h. |
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 350 mm | 90–110 A |
| 3.25 mm | 350 mm | 110–150 A |
| 3.25 mm | 450 mm | 110–150 A |
| 4 mm | 350 mm | 140–180 A |
| 4 mm | 450 mm | 140–180 A |
| 5 mm | 450 mm | 180–220 A |
| 6 mm | 450 mm | 210–270 A |
| Product | Class | Rm | KV | Availability |
|---|---|---|---|---|
| GARANT SKjellberg | E7018-1 | 540–600 MPa | > 90 J (−40 °C) | To order · price and lead time in the quote |
| GARANT XKjellberg | E7018-1 | 550–600 MPa | > 70 J (−20 °C) | To order · price and lead time in the quote |
| LASER B 50Gedik | E7018-1 H4 | 510–630 MPa | min. 47 J (−50 °C) | To order · price and lead time in the quote |
| LASER B 55Gedik | E7018-1 H4 | 530–650 MPa | min. 47 J (−50 °C) | To order · price and lead time in the quote |
| LASER B 55-SGedik | E7018-1 H4 | 530–650 MPa | min. 47 J (−60 °C) | To order · price and lead time in the quote |