Gedik · Stainless steels
ELOX R 385 — E 385 -16
covered electrode · stick electroderutile coating
Choose the size
- Ø 2.5 × 250 mm≈ 5 kg
- Ø 3.2 × 350 mm≈ 5 kg
- Ø 4 × 350 mm≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
7.11–11.36 kg
of ELOX R 385 for 10 m of weld
3 packs of ≈ 5 kg
Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Which filler joins two different metals?With this product's data: 385
Not recommendedFN — (WRC-1992)
- Fully austenitic weld, as expected from a superaustenitic filler (type 385).
- Superaustenitic filler (type 385) with carbon steel: not recommended for this joint; use 309L or 309LMo.
Maximum dilution with this filler: 74.5 %
Calculated with: filler 385 — this product · dilution 30 % typical of 111, equal shares of each metal
See the full calculation →Field of application
- Resistant to intergranular corrosion (wet corrosion up to 350 °C)
- High corrosion resistance, similar to that of matching steels and cast steels, especially in reducing media
- For joining and surfacing matching austenitic CrNiMoCu steels and cast steels
- For joining these steels to non-alloy and low-alloy steels and cast steels
- Redrying is required for at least 2 hours at 120 °C to 200 °C
Base metals
EN & DIN:
X5NiCrMoCuNb 20 18X5NiCrMoCuTi 20 18X2NiCrMoCu 25 20 5X5NiCrMoCuNb 22 18G-X7CrNiMoCuNb 18 18G-X7NiCrMoCuNb 25 20
AISI:
317L904L
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up |
|---|---|
| Polarity | DC+/AC |
Classification and approvals
Classification
| AWS class | E 385 -16 |
|---|---|
| EN ISO class | E 20 25 5 Cu N L R 32 |
Approvals
- TSE, CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | < 0.03 |
|---|---|
| Cr | 20.0 |
| Cu | 1.50 |
| Mn | 1.00 |
| Mo | 4.50 |
| Ni | 25.0 |
| Si | 0.75 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | min. 400 MPa |
|---|---|
| Tensile strength (Rm) | 550–700 MPa |
| Elongation (A5) | min. 30 % |
| Impact energy (KV) | min. 47 J (20 °C) |
| Service temperature | max. 350 °C |
How to weld
Treatment and preparation
| Re-drying | 120–200 °C / min. 2 h |
|---|
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 250 mm | 50–90 A |
| 3.2 mm | 350 mm | 80–120 A |
| 4 mm | 350 mm | 110–160 A |
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
| Product | Class | Rm | KV | Availability |
|---|---|---|---|---|
| FINOX 4519 ACKjellberg | E 20 25 5 Cu N L R 32 | > 550 MPa | > 55 J (room temperature) | To order · price and lead time in the quote |