Gedik · Creep-resisting Cr-Mo steels
ELCOR R CrMo1 FCW — E81 T1-B2C
flux-cored wire (FCW)
Choose the size
- Ø 1.2 mm · BS 300≈ 15 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 136 · η 0.80–0.90
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
5.03–7.66 kg
of ELCOR R CrMo1 FCW for 10 m of weld
1 pack of 15 kg
Calculated with: η 0.80–0.90: typical value for process 136 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Field of application
- Rutile type flux-cored wire
- Typical applications are vessel and steel construction, mechanical engineering and pipe work
- Good arc restriking even with cold wire tip, suitable for robot applications
- Multi-pass welding without in-between cleaning
- Ideal for use in the field short arc and spray arc
- Excellent gap bridging for root welding
- High-efficiency type for economic production environments
- Shielding gas: CO2
Base metals
DIN:
13 CrMo 4424 CrMo 5
Cast Steels: GS 17CrMo55GS 22CrMo54G17CrMo5-5G22CrMo5-4
EN:
13 CrMo 4-5
ASTM:
A 182A 387A217A 387 Gr. 11-12
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up PG vertical-down |
|---|---|
| Polarity | DC+ |
| Shielding gas | CO2 |
Classification and approvals
Classification
| AWS class | E81 T1-B2C |
|---|---|
| EN ISO class | T CrMo1 R C 2 |
Approvals
- CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.06 |
|---|---|
| Cr | 1.20 |
| Mn | 1.20 |
| Mo | 0.50 |
| Si | 0.50 |
Values in mass %.
Mechanical properties
typical values, with M21 gas
after heat treatment: 680 °C / 1 h
| Yield strength (Rp0.2) | min. 460 MPa |
|---|---|
| Tensile strength (Rm) | 550–690 MPa |
| Elongation (A5) | min. 19 % |
| Impact energy (KV) | min. 80 J (room temperature) |
after heat treatment: 920 °C / 30 min
| Yield strength (Rp0.2) | min. 320 MPa |
|---|---|
| Tensile strength (Rm) | 450–550 MPa |
| Elongation (A5) | min. 26 % |
| Impact energy (KV) | min. 100 J (room temperature) |
How to weld
Process
| Shielding | Requires shielding gas |
|---|
FERVEO guidance