Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Dratec · Low-alloy steels

DT-NiMoCr MIG — ER 100S-G

solid wire

Choose the size

  • Ø 0.8 mm · K300 15–20 kg
    ≈ 15 kg
  • Ø 1 mm · K300 15–20 kg
    ≈ 15 kg
  • Ø 1.2 mm · K300 15–20 kg
    ≈ 15 kg
  • Ø 1.6 mm · K300 15–20 kg
    ≈ 15 kg

Indicative diameters; confirmed with the order

Supply programme: spools on request D100 (0.5–1 kg), D200 (2–5 kg)

To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 135 · η 0.92–0.98
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

4.62–6.66 kg

of DT-NiMoCr MIG for 10 m of weld

1 pack of ≈ 15 kg

Calculated with: η 0.92–0.98: typical value for process 135 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

Welding wire for joints on NiMo-alloyed steels in apparatus, vessel and pipeline construction, as well as on high-strength fine-grain structural steels. Quenched and tempered fine-grain steels

Base metals

1.89861.89871.8988St 50-St 70StE51-StE 60S550QL1 (N-A-XTRA 56)S620QL1 (N-A-XTRA 63)S690QL1 ESTE 690 (N-A-XTRA 70)S700MC (PAS 70)
PolarityDC+
Shielding gasM2

Classification and approvals

Classification

AWS classER 100S-G
EN ISO classG 69 4 M21 Mn3Ni1CrMo

Approvals

  • MSG: TÜV
  • DB, CE
According to the Dratec 2025 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the wire

C0.10
V0.10
Cr0.35
Mn1.60
Mo0.30
Ni1.40
Si0.60
Values in mass %.

Mechanical properties

guide values
Yield strength (Rp0.2)> 690 MPa
Tensile strength (Rm)770–940 MPa
Elongation (A5)> 17 %
Impact energy (KV)> 47 J (−40 °C)
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassRmKVAvailability
ER 110 SG G 69 4 MIGGedikG 69 4 M21 Mn3Ni1CrMomin. 760 MPamin. 47 J (−30 °C)To order · price and lead time in the quote
Similar
ISO 16834-A: same strength (69), equal or better toughness (47 J at −40 °C)
ProductClassRmKVAvailability