We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Creep-resisting Cr-Mo steels

CROMO 2B — E 9018-B3

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 350 mm · 4.3 kg
    ≈ 4.3 kg
  • Ø 3.25 × 350 mm · 4.8 kg
    ≈ 4.8 kg
  • Ø 4 × 350 mm · 6 kg
    ≈ 6 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.97–11.14 kg

of CROMO 2B for 10 m of weld

3 packs of 4.3 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

Covered electrode for joining boiler and tube steels and similar CrMo-alloyed steels resistant to hydrogen under pressure, preferably for the creep-resisting steel 10CrMo9-10 at service temperatures up to 600 °C in long-term service. Also suitable for joining and surfacing on similarly alloyed case-hardening and quenched and tempered steels.

Base metals

1.7259 26 CrMo 71.7273 24 CrMo 101.7276 10 CrMo 111.7281 16 CrMo 9-31.7379 G17 CrMo 9-101.7380 10 CrMo 9-101.7382 G19 CrMo 9-101.7383 11 CrMo 9-101.7387 G12 CrMo 9-101.8075 10 CrSiMoV 7ASTM A 335 (P22)
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE 9018-B3
EN ISO classE CrMo2 B 42

Approvals

  • TÜV, CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.08
Cr2.20
Mn0.90
Mo1.10
Si0.40
Values in mass %.

Mechanical properties

after tempering: min. 0.5 h at 700 °C, cooling in still air
Yield strength (Rp0.2)> 400 MPa
Tensile strength (Rm)500–600 MPa
Elongation (A5)> 20 %
Impact energy (KV)> 47 J (20 °C)

How to weld

Treatment and preparation

Re-drying300–350 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm90–110 A
3.25 mm350 mm110–150 A
4 mm350 mm140–180 A
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassAvailability
OPUS 2 CMGedikE CrMo2 B 42 H5To order · price and lead time in the quote
OPUS 2 CM-15GedikE CrMo2 B 42 H5To order · price and lead time in the quote