We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Gedik · Low-alloy steels

TEMPO B 70 S — E 9018 - G H4

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 350 mm
    ≈ 5 kg
  • Ø 3.2 × 350 mm
    ≈ 5 kg
  • Ø 4 × 450 mm
    ≈ 5 kg
  • Ø 5 × 450 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.97–11.14 kg

of TEMPO B 70 S for 10 m of weld

3 packs of ≈ 5 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

  • Suitable for welding high-strength fine-grained steels
  • High ductility and high crack resistance in welds produced in fine-grained steels
  • Suitable for applications involving service temperatures from -60 °C to +350 °C
  • Redrying is required for at least 2 hours at 300 °C to 350 °C

Base metals

S380N-S500NS355NH-S460NHS380NL-500NLFine grainedhigh alloyed steels and steel castings
API 5L:
X52X56X60X65X70
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE 9018 - G H4
EN ISO classE 55 6 2 NiMo BT 42 H5

Approvals

  • CE, ABS, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.07
Mn0.60
Mo0.40
Ni2.40
Si0.20
Values in mass %.

Mechanical properties

after heat treatment: 560–600 °C / 1 h / 300 °C (air)
Yield strength (Rp0.2)min. 550 MPa
Tensile strength (Rm)620–780 MPa
Elongation (A5)min. 18 %
Impact energy (KV)min. 47 J (−60 °C)

How to weld

Treatment and preparation

Re-drying300–350 °C / min. 2 h

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–110 A
3.2 mm350 mm100–140 A
4 mm450 mm130–190 A
5 mm450 mm190–240 A
FERVEO guidance
FERVEO text, not the manufacturer's
What it is for

Basic electrode for joining high-strength fine-grain steels — S380N to S500N, API 5L X52 to X70 pipe — with weld metal that stays tough down to −60 °C.

Typical applications
Pipeline construction[datasheet]Steel construction[datasheet]
By problem
Structural steels
Advantages
  • Tough at −60 °C: 47 J after heat treatment[datasheet · standard · source]
  • H5: diffusible hydrogen ≤ 5 ml/100 g[datasheet · standard]
  • Lower risk of cold cracking when redried as the maker says (2 h at 300–350 °C)[datasheet · source]
  • One electrode for service temperatures from −60 °C to +350 °C[datasheet]
Alternatives in the catalogue
Similar
ISO 18275-A: same strength (55), equal or better toughness (47 J at −60 °C), same covering (B)
ProductClassRmKVAvailability
TEMPO B 65GedikE 55 6 1 NiMo B 42 H5630–750 MPamin. 47 J (−60 °C)To order · price and lead time in the quote
TEMPO B 70 MGedikE 55 6 Z (1 NiMo) B 42 H5To order · price and lead time in the quote