We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Gedik · Low-alloy steels

TEMPO B 70 Mo — ~ E 9018-D1 H4

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 350 mm
    ≈ 5 kg
  • Ø 3.2 × 350 mm
    ≈ 5 kg
  • Ø 4 × 450 mm
    ≈ 5 kg
  • Ø 5 × 450 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.97–11.14 kg

of TEMPO B 70 Mo for 10 m of weld

3 packs of ≈ 5 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Do I need to preheat?With this product's data: H5
Thickness of the thickest part in the jointmethod B: d from 10 to 90 mm

100 °C

Minimum preheat and minimum interpass temperature

EN 1011-2, annex C, method B · rounded up to 5 °C

✓ Within the range of method B.

Calculated with: HD 5 ml/100 g from this product's class H5 · 111 — basic electrode: 24 V, 160 A, 15 cm/min

See the full calculation →

Field of application

  • Suitability for use in welding high-strength, fine-grained constructional steels and high-temperature steels
  • Use in welding rail steels with strength values up to 785 N/mm2
  • Content including MnMo alloy
  • Resistance to cracking as well as to aging, high toughness
  • Requirement of re-drying for minimum 2 hours at the temperatures between 300°C and 350°C

Base metals

E295-E360P355GH17MnMoV6-415NiCuMoNb5SS380N-S500NP380NH-S500NHGE300-GE340G22Mo4
API 5L:
X52X56X60X65X70
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS class~ E 9018-D1 H4
EN ISO classE 55 5 MnMo B 42 H5

Approvals

  • CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.075
Mn1.60
Mo0.45
Si0.40
Values in mass %.

Mechanical properties

after heat treatment: 560–600 °C / 1 h / 300 °C (air)
Yield strength (Rp0.2)min. 550 MPa
Tensile strength (Rm)620–780 MPa
Elongation (A5)min. 18 %
Impact energy (KV)min. 47 J (−50 °C)

How to weld

Treatment and preparation

Re-drying300–350 °C / min. 2 h

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–110 A
3.2 mm350 mm100–140 A
4 mm450 mm130–190 A
5 mm450 mm190–240 A
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Similar
ISO 18275-A: same strength (55), equal or better toughness (47 J at −50 °C), same covering (B)
ProductClassRmKVAvailability
TEMPO B 65GedikE 55 6 1 NiMo B 42 H5630–750 MPamin. 47 J (−60 °C)To order · price and lead time in the quote
TEMPO B 70 MGedikE 55 6 Z (1 NiMo) B 42 H5To order · price and lead time in the quote
TEMPO B 70 SGedikE 55 6 2 NiMo BT 42 H5To order · price and lead time in the quote