Gedik · Low-alloy steels
TEMPO B 3 — E 8018-C2 H4
covered electrode · stick electrodebasic coating
Choose the size
- Ø 2.5 × 350 mm≈ 5 kg
- Ø 3.2 × 350 mm≈ 5 kg
- Ø 4 × 450 mm≈ 5 kg
- Ø 5 × 450 mm≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 111 · η 0.62
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
7.25–9.81 kg
of TEMPO B 3 for 10 m of weld
2 packs of ≈ 5 kg
Calculated with: η 0.62 — from the datasheet (recovery 120 %, Ø 2.5 × 350 mm) · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Do I need to preheat?With this product's data: H5
Thickness of the thickest part in the jointmethod B: d from 10 to 90 mm
100 °C
Minimum preheat and minimum interpass temperature
EN 1011-2, annex C, method B · rounded up to 5 °C
✓ Within the range of method B.
Calculated with: HD 5 ml/100 g from this product's class H5 · 111 — basic electrode: 24 V, 160 A, 15 cm/min
See the full calculation →Field of application
- Suitability for use in welding Ni-alloyed construction steels for cryogenic applications
- High ductility and crack resistance in weld deposits
- Serviceability of weld metals at temperatures down to -110°C
- Weld metal recovery of approx. 120%
- Convenience of welding at all positions except for vertical down position
- Weld deposits with very low contents of hydrogen
- Requirement of re-drying for minimum 2 hours at the temperatures between 300°C and 350°C
Base metals
Cold-tough steels: 10 Ni1416Ni16S 255NL1-SS00NL1S275NL2-P460NL2
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up |
|---|---|
| Polarity | DC+ |
Classification and approvals
Classification
| AWS class | E 8018-C2 H4 |
|---|---|
| EN ISO class | E 46 6 3 Ni B 42 H5 |
Approvals
- TSE, CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.05 |
|---|---|
| Mn | 0.70 |
| Ni | 3.20 |
| Si | 0.30 |
Values in mass %.
Mechanical properties
after heat treatment: 605 °C / 2 h / 300 °C (air)
| Yield strength (Rp0.2) | min. 460 MPa |
|---|---|
| Tensile strength (Rm) | 550–700 MPa |
| Elongation (A5) | min. 24 % |
| Impact energy (KV) | min. 47 J (−100 °C) |
How to weld
Process
| Recovery | approx. 120 % |
|---|
Treatment and preparation
| Re-drying | 300–350 °C / min. 2 h |
|---|
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 350 mm | 70–110 A |
| 3.2 mm | 350 mm | 110–140 A |
| 4 mm | 450 mm | 140–180 A |
| 5 mm | 450 mm | 190–230 A |
FERVEO guidance
By problem
Structural steels