We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Gedik · Low-alloy steels

SG NiMo1 MIG — ER 100 S-G

solid wire

Choose the size

  • Ø 1.2 mm · BS 300 spool
    ≈ 15 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 135 · η 0.92–0.98
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

4.62–6.66 kg

of SG NiMo1 MIG for 10 m of weld

1 pack of 15 kg

Calculated with: η 0.92–0.98: typical value for process 135 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

  • Fine-grained low alloy steels and also austempering steels for applications. Building up of cranes, transport, tanks, industrial facilities, equipment in general, pipelines, shipbuilding, etc
  • If necessary, post-weld stress relief shall be heat treated at 560°C-600°C for 1 hour and left in the furnace for cooling down to 300°C
  • Shielding gas: Ar+CO2 mix gases can be used

Base metals

P355NL1P460NL1StE460-590USS-T.TTSTE47-51N-X-ATRA 70WTSt37-2WT37-3WTSt52-3WT St52-3APatinax 37Alcodur 50Koralpin 52S255S550A516A350A612A255A299A333
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up PG vertical-down
PolarityDC+
Shielding gasAr + CO2

Classification and approvals

Classification

AWS classER 100 S-G
EN ISO classG 62 6 C1/M21 Mn3Ni1Mo

Approvals

  • CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the wire

C0.09
Mn1.70
Mo0.40
Ni1.15
Si0.65
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)min. 620 MPa
Tensile strength (Rm)700–890 MPa
Elongation (A5)min. 18 %
Impact energy (KV)min. 47 J (−60 °C)

How to weld

Process

ShieldingRequires shielding gas

Treatment and preparation

Post-weld heat treatment560–600 °C / 1 h / furnace down to 300 °C, if necessary
FERVEO guidance
By problem
Structural steels
Alternatives in the catalogue
Similar
ISO 16834-A: same strength (62), equal or better toughness (47 J at −60 °C)
ProductClassRmKVAvailability
DT-NiMo MIGDratecG 62 6 M/C Mn3Ni1Mo700–890 MPa> 47 J (−60 °C)To order · price and lead time in the quote