Choose the size
- Ø 0.8 mm · BS 300≈ 15 kg
- Ø 0.8 mm · D 300≈ 15 kg
- Ø 1 mm · BS 300≈ 15 kg
- Ø 1 mm · D 300≈ 15 kg
- Ø 1.2 mm · BS 300≈ 15 kg
- Ø 1.2 mm · D 300≈ 15 kg
- Ø 1.6 mm · BS 300≈ 15 kg
- Ø 1.6 mm · D 300≈ 15 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 135 · η 0.92–0.98
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
4.62–6.66 kg
of SG CrMo 2 MIG for 10 m of weld
1 pack of 15 kg
Calculated with: η 0.92–0.98: typical value for process 135 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Field of application
- Used for the welding of high heat resisting
- XCr-Mo alloyed steels which are used for the production of boilers tubes, pipes and nitrided steels
- Weld metal is resistant to temperatures up to +600°C
- Shielding gases: MAG; Ar+CO2 and Ar+O2 mix gases, TIG; pure Ar gas can be used
Base metals
10 CrMo9-1010 CrSiMoV 710 CrV 63G-17 CrMo 9-10A335 Gr. P22
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up PG vertical-down |
|---|---|
| Polarity | DC+ |
| Shielding gas | Ar + CO2, Ar + O2 |
Classification and approvals
Classification
| AWS class | ER 90 S-B3 |
|---|---|
| EN ISO class | G Z CrMo 2 Si |
Approvals
- CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the wire
| C | 0.08 |
|---|---|
| Cr | 2.40 |
| Mn | 0.50 |
| Mo | 1.00 |
| Si | 0.60 |
Values in mass %.
Mechanical properties
after heat treatment: 690 °C / 1 h / 300 °C (air)
| Yield strength (Rp0.2) | min. 540 MPa |
|---|---|
| Tensile strength (Rm) | 620–760 MPa |
| Elongation (A5) | min. 20 % |
| Impact energy (KV) | min. 47 J (20 °C) |
How to weld
Process
| Shielding | Requires shielding gas |
|---|
FERVEO guidance
By problem
Structural steels