Gedik · Creep-resisting Cr-Mo steels

SG CrMo 1 TIG — ER 80 S-B2

TIG rod
also as: solid wire

Choose the size

  • Ø 1.6 × 1000 mm · 5 kg
    ≈ 5 kg
  • Ø 2 × 1000 mm · 5 kg
    ≈ 5 kg
  • Ø 2.4 × 1000 mm · 5 kg
    ≈ 5 kg
  • Ø 3.2 × 1000 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 1000 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 141 · η 0.94
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

4.82–6.52 kg

of SG CrMo 1 TIG for 10 m of weld

2 packs of 5 kg

Calculated with: η 0.9405: TIG with filler rod, 0.99 less the stub s of a 1000 mm rod · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

  • Used for the welding of high heat resisting. Cr-Mo alloyed steels which are used for the production of boilers tubes and pipes and nitrided steels
  • Weld metal is resistant to temperatures up to +570°C
  • Shielding gases: MAG; Ar+CO2 and Ar+ O2 mix gases, TIG; pure Ar gas can be used

Base metals

13CrMo4-515CrMo542CrMo416CrMoV425CrMo424CrMo5G22CrMo5-4G17CrMo5-5A 333GrP11
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up PG vertical-down
PolarityDC−
Shielding gas100% Ar

Classification and approvals

Classification

AWS classER 80 S-B2
EN ISO classW Z CrMo1 Si

Approvals

  • CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the wire

C0.10
Cr1.20
Mn0.50
Mo0.50
Si0.60
Values in mass %.

Mechanical properties

after heat treatment: 620 °C / 1 h / 300 °C (air)
Yield strength (Rp0.2)min. 470 MPa
Tensile strength (Rm)550–670 MPa
Elongation (A5)min. 19 %
Impact energy (KV)min. 47 J (20 °C)

How to weld

Process

ShieldingRequires shielding gas
FERVEO guidance
By problem