FINOX 4551 AC — E 347-16

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2.5 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

7.02–11.21 kg

of FINOX 4551 AC for 10 m of weld

3 packs of 4 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Which filler joins two different metals?With this product's data: 347

Not recommendedFN — (WRC-1992)

  • The weld sits close to the martensite boundary: keep the dilution under control.
  • Fully austenitic: sensitive to hot cracking.

Maximum dilution with this filler: 10.5 %

Calculated with: filler 347 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Electrode for joining unstabilised and stabilised austenitic corrosion-resisting CrNi steels at service temperatures up to 400 °C, for corrosion-resisting Cr steels and for claddings of similar composition.

Base metals

1.4301 X 5 CrNi 18-101.4306 X 2 CrNi 19-111.4311 X 2 CrNiN 18-101.4541 X 6 CrNiTi 18-101.4550 X 6 CrNiNb 18-101.4552 GX 5 CrNiNb 19-11
AISI:
304304L304LN321347
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS classE 347-16
EN ISO classE 19 9 Nb R 12
Material no. (W.-Nr.)1.4551

Approvals

  • DB, TÜV, CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.02
Cr19.0
Mn0.80
Nb0.30
Ni9.50
Si0.90
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 350 MPa
Tensile strength (Rm)> 550 MPa
Elongation (A5)> 25 %
Impact energy (KV)> 55 J (room temperature)

How to weld

Treatment and preparation

Re-drying300–350 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm300 mm80–100 A
3.25 mm350 mm100–130 A
4 mm350 mm120–160 A
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same AWS designation
ProductClassRmKVAvailability
ELOX R 347GedikE347-16570–740 MPamin. 47 J (20 °C)To order · price and lead time in the quote