We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Stainless steels

FINOX 4337 AC — E 312-16

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 2.5 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Which filler joins two different metals?With this product's data: 312

SuitableFN 22.7 (WRC-1992)

✓

Maximum dilution with this filler: 57.5 %

Calculated with: filler 312 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Electrode for joining and surfacing on matching and similar steels and cast steels, for joining higher-strength non-alloy and low-alloy structural steels, quenched and tempered steels, tool steels and austenitic manganese steel, and for joining dissimilar steels to each other and to high-alloy stainless steels. The electrode is also suitable for crack-resistant, hard and tough intermediate layers under hardfacing, and for hardfacing deposits, work-hardenable when cold and hot. The austenitic-ferritic weld metal is stainless, corrosion-resisting and suitable for service temperatures up to 300 °C. Owing to the higher delta-ferrite content of the weld metal, dissimilar joints between ferritic and austenitic steels have high resistance to hot cracking.

PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS classE 312-16
EN ISO classE 29 9 R 12
Material no. (W.-Nr.)1.4337

Approvals

  • CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.10
Cr29.0
Mn1.00
Ni9.00
Si0.90
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 500 MPa
Tensile strength (Rm)> 700 MPa
Elongation (A5)> 20 %

How to weld

Treatment and preparation

Re-drying300–350 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2 mm300 mm50–70 A
2.5 mm300 mm70–100 A
3.25 mm350 mm100–140 A
4 mm350 mm130–170 A
FERVEO guidance
By problem
Dissimilar metalsStainless steel and dissimilar metalsI don't know what steel the part isCorrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassRmKVAvailability
299 SUPERGedikE 29 9 R 12790–860 MPaTo order · price and lead time in the quote
ELOX R 312GedikE 29 9 R 12700–830 MPamin. 24 J (20 °C)To order · price and lead time in the quote