We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Stainless steels

FINOX 4332 AC — E 309 L-16

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2.5 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

7.02–11.21 kg

of FINOX 4332 AC for 10 m of weld

3 packs of 4 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Which filler joins two different metals?With this product's data: 309L

With reservationsFN 2.1 (WRC-1992)

  • Ferrite below 3 FN: risk of hot cracking (API RP 582, TWI).

Maximum dilution with this filler: 25.5 %

Calculated with: filler 309L — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Electrode for joining non-alloy and low-alloy steels to high-alloy steels and cast steels, for dissimilar joints between austenitic and ferritic steels at service temperatures up to 300 °C, for welding buffer layers and claddings that are corrosion-resisting already in the first layer, and for welding the transition zones of CrNi-clad plates.

PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS classE 309 L-16
EN ISO classE 23 12 L R 32
Material no. (W.-Nr.)1.4332

Approvals

  • CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.02
Cr23.0
Mn0.70
Ni13.0
Si0.90
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 380 MPa
Tensile strength (Rm)> 550 MPa
Elongation (A5)> 30 %
Impact energy (KV)> 55 J (room temperature)

How to weld

Treatment and preparation

Re-drying300–350 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm300 mm80–100 A
3.25 mm350 mm100–130 A
4 mm350 mm120–160 A
FERVEO guidance
By problem
Dissimilar metalsStainless steel and dissimilar metalsCorrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassRmKVAvailability
ELOX R 309 LGedikE 23 12 L R 32540–720 MPamin. 47 J (20 °C)To order · price and lead time in the quote
ELOX R 309 L-17GedikE 23 12 L R 32540–720 MPamin. 47 J (20 °C)To order · price and lead time in the quote