We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Nickel alloys

FINOX 182 — E NiCrFe-3

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Which filler joins two different metals?With this product's data: Ni 6182

Suitable

The Schaeffler diagram does not apply to a nickel-base weld; the service assessment is shown.

✓

Calculated with: filler Ni 6182 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Nickel-base electrode for high-quality, crack-resistant joining and cladding on matching nickel-chromium-iron alloys, (heat-resisting) Cr and CrNi (Mo, N) steels and nickel-alloyed pressure vessel steels tough at low temperatures. For dissimilar joints between austenitic and ferritic steels (e.g. 1.4583 with 16Mo3). Use at service temperatures from -196 °C up to 800 °C. (In sulphur-containing atmospheres only up to 500 °C). The fully austenitic weld metal is corrosion-resisting, tough at low temperatures, with high-temperature strength, resistant to scaling up to 1,000 °C and not susceptible to embrittlement.

Base metals

1.4876 X 10 NiCrAlTi 32-212.4816 NiCr 15 FeAlloy 600Alloy 800
PositionsPA flat PB horizontal-vertical PC horizontal PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS classE NiCrFe-3
EN ISO class≈ E Ni 6182 (NiCr15Fe6Mn)
Material no. (W.-Nr.)2.4620

Composition and properties

Chemical composition of the weld metal

C0.05
Cr16.0
Fe8.00
Mn6.00
Mo1.00
Nb2.00
Nibalance
Si0.50
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 350 MPa
Tensile strength (Rm)> 620 MPa
Elongation (A5)> 35 %
Impact energy (KV)> 90 J (room temperature)

How to weld

Treatment and preparation

Re-drying150–200 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm350 mm80–110 A
3.25 mm350 mm110–140 A
4 mm350 mm140–180 A
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same AWS designation
ProductClassRmKVAvailability
NIBAZ B 71GedikE NiCrFe3min. 550 MPamin. 47 J (20 °C)To order · price and lead time in the quote