Kjellberg · Cast iron
FICAST NIFE BAL — E NiFe-CI-A
covered electrode · stick electrode
Choose the size
- Ø 3.25 × 350 mm · 1.5 kg≈ 1.5 kg
- Ø 4 × 350 mm · 1.5 kg≈ 1.5 kg
To order · price and lead time in the quote
We reply within 1 working day.
Field of application
Special electrode for cold welding of grey cast iron with lamellar graphite, spheroidal graphite cast iron and malleable cast iron, also suitable for joining cast iron (GGL and GGG grades) to non-alloy steels. The higher Al content gives improved welding characteristics, with higher resistance to porosity but lower toughness than FICAST NiFe and FICAST NiFe B. The bimetallic core wire ensures a stable arc, good wetting and, as it withstands high welding currents, a higher deposition rate. The weld metal is machinable and is characterised by high crack resistance.
| Positions | PA flat PB horizontal-vertical PC horizontal PF vertical-up |
|---|---|
| Polarity | DC±/AC |
Classification and approvals
Classification
| AWS class | E NiFe-CI-A |
|---|---|
| EN ISO class | E C NiFe-CI A1 |
Composition and properties
Chemical composition of the weld metal
| C | 1.30 |
|---|---|
| Al | present |
| Fe | 47.0 |
| Mn | 0.70 |
| Ni | 50.0 |
| Si | 0.70 |
Values in mass %.
Mechanical properties
| Tensile strength (Rm) | > 450 MPa |
|---|
Hardness
- 180 HB
How to weld
Treatment and preparation
| Re-drying | 100–150 °C / 1 h |
|---|
Storage
In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.
| Moisture in the covering | More spatter and porosity: redry, above all when low hydrogen content is required. |
|---|
According to the Kjellberg 2019 catalogue
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 3.25 mm | 350 mm | 90–110 A |
| 4 mm | 350 mm | 110–150 A |
FERVEO guidance
By problem
Cast iron