Nickel alloys

FERVEO NIC 825 TIG

TIG rodCatalogue only
also as: solid wire
AWS class
ERNiFeCr-1
EN ISO class
EN ISO 18274: S Ni 8065 – NiFe30Cr21Mo3
Tensile strength (Rm)
550 MPa

Classification

AWS classERNiFeCr-1
EN ISO classEN ISO 18274: S Ni 8065 – NiFe30Cr21Mo3
Material no. (W.-Nr.)2.4858

Purpose

  • Fe-Ni-Cr-Mo-Cu solid TIG rod (alloy 825) for joining and surfacing alloy 825 and CrNiMoCu austenitic steels.
  • Good corrosion resistance in sulfuric and phosphoric acid media.

Why it works

Copper (2.5%) added to an Fe-Ni-Cr-Mo base is what sets this alloy apart — like the copper in CUP 28 (the INX superaustenitic line), it specifically improves behavior against sulfuric acid, while molybdenum (3.1%) provides pitting resistance in chlorides.

Fields of application

  • Joining and surfacing alloy 825 (2.4858, UNS N08825).
  • CrNiMoCu austenitic steels in process equipment handling sulfuric or phosphoric acid.

Chemical composition

ElementTypical, %
C0.01
Cr22.5
Cu2.5
Febalance
Mn0.8
Mo3.1
Ni44
Si0.3
Ti0.9

Mechanical properties

Tensile strength (Rm)550 MPa
Yield strength (Rp0.2)360 MPa
Elongation (A5)30 %
Impact energy (KV)100 J

Process

PolarityDC−
Shielding gasI1

Sizes and part numbers

ØRequest
1 mm
1.6 mm
2.4 mm
3.2 mm

Supply programme

boxes 5 / 10 kg

Base metals

2.4858 (Alloy 825, UNS N08825)UNS N08904

Advantages

  • Copper (2.5%) specifically improves resistance to sulfuric and phosphoric acid.
  • Good strength-ductility balance (Rm 550 MPa, A5 30%).

Limitations

  • Supplier datasheet gives no shielding-gas data (MIG or TIG) — confirm parameters with the manufacturer before welding.
  • Iron-base alloy (not nickel-base) — lower high-temperature resistance than this datasheet's NiCr/NiCrMo alloys.

Notes