Gedik · Stainless steels
ELOX BS 410 Ni Mo — E 410NiMo-25
covered electrode · stick electrodebasic coating
Choose the size
- Ø 2.5 × 350 mm≈ 5 kg
- Ø 3.2 × 350 mm≈ 5 kg
- Ø 4 × 350 mm≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
Field of application
- Electrode with a basic covering for welding similar corrosion-resisting martensitic and martensitic-ferritic rolled, forged and cast steels
- For hydraulic turbines, compressors and steam power plants
- Resistant to corrosion by water, steam and seawater atmospheres
- Excellent slag removal and a smooth bead appearance
- Metal recovery approx. 130 %; suitable for positional welding
- Preheating and interpass temperature for thick-walled components: 100 °C to 160 °C
- Tempering temperature: 580 °C to 620 °C
- Redrying is required for at least 2 hours at 300 °C to 350 °C
Base metals
X5CrNi 13 4G-X5CrNi 13 4X6Cr 13G-X5CrNi 13 6
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up |
|---|---|
| Polarity | DC+ |
Classification and approvals
Classification
| AWS class | E 410NiMo-25 |
|---|---|
| EN ISO class | E 13 4 B 62 |
Approvals
- TSE, CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.05 |
|---|---|
| Cr | 11.5 |
| Mn | 0.50 |
| Mo | 0.50 |
| Ni | 4.50 |
| Si | 0.30 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | min. 600 MPa |
|---|---|
| Tensile strength (Rm) | 800–980 MPa |
| Elongation (A5) | min. 15 % |
| Impact energy (KV) | min. 47 J (20 °C) |
Hardness
- approx. 270 HB
How to weld
Process
| Recovery | approx. 130 % |
|---|
Treatment and preparation
| Re-drying | 300–350 °C / min. 2 h |
|---|---|
| Pre-heating | 100–160 °C, for thick-walled components |
| Interpass temperature | 100–160 °C, for thick-walled components |
| Post-weld heat treatment | 580–620 °C |
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 350 mm | 70–110 A |
| 3.2 mm | 350 mm | 110–150 A |
| 4 mm | 350 mm | 150–190 A |
FERVEO guidance
By problem
Corrosion-resistant alloys