We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Gedik · Stainless steels

ELOX B 410 — E 410-15

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 250 mm
    ≈ 5 kg
  • Ø 3.2 × 350 mm
    ≈ 5 kg
  • Ø 4 × 350 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Field of application

  • 13 % Cr electrode for joining and surfacing martensitic and martensitic-ferritic 13 % Cr steels and cast steels (also suitable for surfacing the sealing faces of gas, water and steam valves)
  • Annealing at 750 °C for 2 hours, then furnace cooling to room temperature
  • Redrying is required for at least 2 hours at 300 °C to 350 °C

Base metals

X6Cr 13X6CrAl 13X15Cr 13X10Cr 13G-X10Cr 13
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS classE 410-15
EN ISO classE 13 B 22

Approvals

  • TSE, CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.07
Cr13.5
Mn0.80
Si0.70
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)min. 450 MPa
Tensile strength (Rm)650–800 MPa
Impact energy (KV)min. 15 J (20 °C)

Hardness

  • as welded — approx. 350 HB
  • after annealing: 750 °C / 2 h / furnace — 200 HB

How to weld

Treatment and preparation

Re-drying300–350 °C / min. 2 h

Welding parameters by diameter

ØLengthCurrent
2.5 mm250 mm50–90 A
3.2 mm350 mm80–120 A
4 mm350 mm110–160 A
FERVEO guidance
By problem
Corrosion-resistant alloys