Choose the size
- Ø 1 mm · box 5 kg≈ 5 kg
- Ø 1.6 mm · box 5 kg≈ 5 kg
- Ø 2 mm · box 5 kg≈ 5 kg
- Ø 2.4 mm · box 5 kg≈ 5 kg
- Ø 3.2 mm · box 5 kg≈ 5 kg
Indicative diameters; confirmed with the order
To order · price and lead time in the quote
We reply within 1 working day.
Which filler joins two different metals?With this product's data: 385
Not recommendedFN — (WRC-1992)
- Fully austenitic weld, as expected from a superaustenitic filler (type 385).
- Superaustenitic filler (type 385) with carbon steel: not recommended for this joint; use 309L or 309LMo.
Maximum dilution with this filler: 74.5 %
Calculated with: filler 385 — this product · dilution 30 % typical of 141, equal shares of each metal
See the full calculation →Field of application
For joining matching austenitic CrNiMoCu steels and cast steels. Good corrosion resistance in reducing media. Resistant to intergranular corrosion (wet corrosion up to approx. 350 °C).
Base metals
1.45001.45051.45061.45361.4539
| Polarity | DC− |
|---|---|
| Shielding gas | I1 |
Classification and approvals
Classification
| AWS class | ER 385 |
|---|---|
| EN ISO class | W 20 25 5 Cu L |
| Material no. (W.-Nr.) | 1.4519 |
| ISO 14343-B | SS385 |
Approvals
- TÜV, DB, CE
According to the Dratec 2025 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the wire
| C | 0.02 |
|---|---|
| Cr | 20.0 |
| Cu | 1.50 |
| Mn | 2.00 |
| Mo | 4.50 |
| Ni | 25.0 |
| Si | 0.20 |
Values in mass %.
Mechanical properties
guide values
| Yield strength (Rp0.2) | 380 MPa |
|---|---|
| Tensile strength (Rm) | 560 MPa |
| Elongation (A5) | 35 % |
| Impact energy (KV) | 80 J |
| Service temperature | −196–350 °C |
FERVEO guidance
By problem
Corrosion-resistant alloys