We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Dratec · Stainless steels

DT-1.4519 MIG — ER 385

solid wire
also as: TIG rod

Choose the size

  • Ø 0.8 mm · K300 15–20 kg
    ≈ 15 kg
  • Ø 1 mm · K300 15–20 kg
    ≈ 15 kg
  • Ø 1.2 mm · K300 15–20 kg
    ≈ 15 kg
  • Ø 1.6 mm · K300 15–20 kg
    ≈ 15 kg

Indicative diameters; confirmed with the order

Supply programme: spools on request D100 (0.5–1 kg), D200 (2–5 kg)

To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 135 · η 0.92–0.98
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

4.71–6.79 kg

of DT-1.4519 MIG for 10 m of weld

1 pack of ≈ 15 kg

Calculated with: η 0.92–0.98: typical value for process 135 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Which filler joins two different metals?With this product's data: 385

Not recommendedFN — (WRC-1992)

  • Fully austenitic weld, as expected from a superaustenitic filler (type 385).
  • Superaustenitic filler (type 385) with carbon steel: not recommended for this joint; use 309L or 309LMo.

Maximum dilution with this filler: 74.5 %

Calculated with: filler 385 — this product · dilution 20 % typical of 135, equal shares of each metal

See the full calculation →

Field of application

For joining matching austenitic CrNiMoCu steels and cast steels. Good corrosion resistance in reducing media. Resistant to intergranular corrosion (wet corrosion up to approx. 350 °C).

Base metals

1.45001.45051.45061.45361.4539
PolarityDC+
Shielding gasM12

Classification and approvals

Classification

AWS classER 385
EN ISO classG 20 25 5 Cu L
Material no. (W.-Nr.)1.4519
ISO 14343-BSS385

Approvals

  • TÜV, DB, CE
According to the Dratec 2025 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the wire

C0.02
Cr20.0
Cu1.50
Mn2.00
Mo4.50
Ni25.0
Si0.20
Values in mass %.

Mechanical properties

guide values
Yield strength (Rp0.2)380 MPa
Tensile strength (Rm)560 MPa
Elongation (A5)35 %
Impact energy (KV)80 J
Service temperature−196–350 °C
FERVEO guidance
By problem
Corrosion-resistant alloys