Gedik · Copper, brasses and bronzes
S4 L TIG — ER CuSn-A
TIG rod
Choose the size
- Ø 2 × 1000 mm · 5 kg≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 141 · η 0.94
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
5.40–7.31 kg
of S4 L TIG for 10 m of weld
2 packs of 5 kg
Calculated with: η 0.9405: TIG with filler rod, 0.99 less the stub s of a 1000 mm rod · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Field of application
- Highly wear resistant, good anti-friction properties suitable for joining copper-zinc alloys and coating of cast irons and steel materials and dissimilar materials like as steel and bronze
- Applications include bearing faces, art bronze, axle bearing
- Shielding Gas for TIG Welding: Ar
- Normal flame must be chosen
- 100 - 250°C pre-heat temperature must be done thicker than 10 mm materials
| Shielding gas | Ar |
|---|
Classification and approvals
Classification
| AWS class | ER CuSn-A |
|---|---|
| EN ISO class | Cu 922 |
| Welding process | gas welding · TIG welding |
Approvals
- SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| P | 0.20 |
|---|---|
| Cu | balance |
| Sn | 6.00 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | 150 MPa |
|---|---|
| Tensile strength (Rm) | 300 MPa |
| Elongation (A5) | 20 % |
Hardness
- 80 HB
How to weld
Process
| Shielding | Requires shielding gas |
|---|
Treatment and preparation
| Pre-heating | 100–250 °C, for materials thicker than 10 mm |
|---|
FERVEO guidance
By problem
Copper and bronze
Alternatives in the catalogue
Same class
same AWS designation
| Product | Class | Rm | Availability |
|---|---|---|---|
| DT-CuSn6 TIGDratec | ERCuSn-A | 300 MPa | To order · price and lead time in the quote |