Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Nickel alloys

FINOX 82 — ≈ E NiCrFe-3

covered electrode · stick electrodebasic coating

Choose the size

  • Ø 2.5 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

Which filler joins two different metals?With this product's data: Ni 6082

Suitable

The Schaeffler diagram does not apply to a nickel-base weld; the service assessment is shown.

✓

Calculated with: filler Ni 6082 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Nickel-base electrode for high-quality, crack-resistant joining and cladding on matching nickel-chromium and nickel-chromium-iron alloys, (heat-resisting) Cr and CrNi (Mo, N) steels and nickel-alloyed pressure vessel steels tough at low temperatures. For dissimilar joints between austenitic and ferritic steels (e.g. 1.4583 with 16 Mo3) – use at service temperatures from -196 °C up to 800 °C (in sulphur-containing atmospheres only up to 500 °C). The electrode is well suited to positional welding. The fully austenitic weld metal is corrosion-resisting, tough at low temperatures, with high-temperature strength, resistant to scaling up to 1,000 °C and not susceptible to embrittlement.

Base metals

1.4876 X 10 NiCrAlTi 32-212.4631 NiCr 20 TiAl2.4669 NiCr 15 Fe 7 TiAl2.4816 NiCr 15 FeAlloy 600Alloy 800Alloy 80AAlloy X750
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+

Classification and approvals

Classification

AWS class≈ E NiCrFe-3
EN ISO classE Ni 6082 (NiCr20Mn3Nb)
Material no. (W.-Nr.)2.4648

Composition and properties

Chemical composition of the weld metal

C0.03
Cr19.0
Fe3.00
Mn5.00
Mo1.50
Nb2.20
Nibalance
Si0.40
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 400 MPa
Tensile strength (Rm)> 620 MPa
Elongation (A5)> 35 %
Impact energy (KV)> 90 J (room temperature)

How to weld

Treatment and preparation

Re-drying250–300 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm300 mm70–100 A
3.25 mm350 mm100–130 A
4 mm350 mm120–160 A
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
ProductClassRmKVAvailability
NIBAZ B 70GedikE Ni 6082 (NiCr20Mn3Nb)630–710 MPamin. 60 J (20 °C)To order · price and lead time in the quote