We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Stainless steels

FINOX 4842 AC — ≈ E 310-16

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2.5 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

7.02–11.21 kg

of FINOX 4842 AC for 10 m of weld

3 packs of 4 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Which filler joins two different metals?With this product's data: 310

Not recommendedFN — (WRC-1992)

  • Fully austenitic: sensitive to hot cracking.
  • Filler 310 gives a fully austenitic weld: with carbon-steel dilution it is prone to hot cracking. For this joint use 309L or 312.

Calculated with: filler 310 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Electrode for joining and surfacing on matching or similar heat-resisting CrNi steels and cast steels for service temperatures up to 1,200 °C, for tough joints and for intermediate and filling runs when welding Cr steels and cast steels. Also suitable for joining non-alloy and low-alloy steels and cast steels, or stainless and heat-resisting Cr steels and cast steels, to austenitic steels and cast steels for service temperatures up to 300 °C. The weld metal does not have sufficient resistance to reducing, sulphur-containing and carburising gases. In these cases, the capping run must be welded with FINOX 4820 AC.

Base metals

1.4710 GX 30 CrSi 71.4713 X 10 CrAlSi 71.4724 X 10 CrAlSi131.4742 X 10 CrAlSi181.4762 X 10 CrAlSi 251.4828 X 15 CrNiSi 20-121.4833 X 12 CrNi 23-131.4840 GX 15 CrNi 25-201.4841 X 15 CrNiSi 25-211.4845 X 8 CrNi 25-211.4846 X 40 CrNi 25-21AISI 310, 310S, 314
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS class≈ E 310-16
EN ISO classE 25 20 R 12
Material no. (W.-Nr.)1.4842

Composition and properties

Chemical composition of the weld metal

C0.12
Cr25.0
Mn3.00
Ni20.0
Si0.70
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 350 MPa
Tensile strength (Rm)> 550 MPa
Elongation (A5)> 30 %
Impact energy (KV)> 70 J (room temperature)

How to weld

Treatment and preparation

Re-drying300–350 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm300 mm80–100 A
3.25 mm350 mm110–140 A
4 mm350 mm130–170 A
FERVEO guidance
By problem
Corrosion-resistant alloys