We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Stainless steels

FINOX 4576 AC — E 318-16

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 2.5 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 5 × 450 mm · 6 kg
    ≈ 6 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

7.11–11.36 kg

of FINOX 4576 AC for 10 m of weld

3 packs of 4 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

Electrode for joining unstabilised and stabilised austenitic corrosion-resisting CrNiMo steels at service temperatures up to 400 °C, for corrosion-resisting Cr steels and for claddings of similar composition.

Base metals

1.4401 X 5 CrNiMo 17-12-21.4404 X 2 CrNiMo 17-12-21.4406 X 2 CrNiMoN 17-11-21.4408 GX 5 CrNiMo 19-11-21.4409 GX 2 CrNiMo 19-11-21.4429 X 2 CrNiMoH 17-13-31.4435 X 2 CrNiMo 18-14-31.4436 X 3 CrNiMo 17-13-31.4571 X 6 CrNiMoTi 17-12-21.4580 X 6 CrNiMo- Nb 17-12-21.4581 GX5 CrNiMo -Nb 19-11-21.4583 X10 CrNiMo- Nb 18-12
AISI:
316316L316 Cb316Ti
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS classE 318-16
EN ISO classE 19 12 3 Nb R 12
Material no. (W.-Nr.)1.4576

Approvals

  • DB, TÜV, DNV-GL, CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.03
Cr18.5
Mn0.80
Mo2.70
Nb0.30
Ni11.5
Si0.90
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 380 MPa
Tensile strength (Rm)> 550 MPa
Elongation (A5)> 30 %
Impact energy (KV)> 55 J (room temperature)

How to weld

Treatment and preparation

Re-drying300–350 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2 mm300 mm60–80 A
2.5 mm300 mm80–100 A
3.25 mm350 mm100–130 A
4 mm350 mm120–160 A
5 mm450 mm160–200 A
FERVEO guidance
By problem
Corrosion-resistant alloys