We open on 1 January 2027. Until then we are not accepting registrations or requests.
Datasheetas published in the maker's catalogueCross-referencesacross makers and AWS / EN ISO classesDeliverySpain and PortugalESPTEN
FERVEO
Basket
Kjellberg · Duplex stainless steels

FINOX 4462 AC — E 2209-17

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2.5 × 300 mm · 4 kg
    ≈ 4 kg
  • Ø 3.25 × 350 mm · 5 kg
    ≈ 5 kg
  • Ø 4 × 350 mm · 5 kg
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

6.93–11.07 kg

of FINOX 4462 AC for 10 m of weld

3 packs of 4 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →
Which filler joins two different metals?With this product's data: 2209

SuitableFN 10.9 (WRC-1992)

✓

Maximum dilution with this filler: 46.5 %

Calculated with: filler 2209 — this product · dilution 30 % typical of 111, equal shares of each metal

See the full calculation →

Field of application

Electrode for joining corrosion-resisting duplex stainless steels. The austenitic weld metal has a ferrite content from approximately 40 up to 50 % and is particularly resistant to pitting corrosion and stress corrosion cracking.

Base metals

1.4460 X 3 CrNiMoN 27-5-21.4462 X 2 CrNiMoN 22-5-31.4463 GX 6 CrNiMo 24-8-21.4582 X 4 CrNiMoNb 25-7
PositionsPA flat PB horizontal-vertical PC horizontal PE overhead PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS classE 2209-17
EN ISO classE 22 9 3 N L R 12
Material no. (W.-Nr.)1.4462

Approvals

  • CE
According to the Kjellberg 2019 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.03
N0.12
Cr22.0
Mn1.00
Mo3.00
Ni9.00
Si0.90
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)> 500 MPa
Tensile strength (Rm)> 700 MPa
Elongation (A5)> 25 %
Impact energy (KV)> 50 J (room temperature)

How to weld

Treatment and preparation

Re-drying300–350 °C / 2 h

Storage

In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.

Moisture in the coveringMore spatter and porosity: redry, above all when low hydrogen content is required.
According to the Kjellberg 2019 catalogue

Welding parameters by diameter

ØLengthCurrent
2.5 mm300 mm70–100 A
3.25 mm350 mm100–130 A
4 mm350 mm120–160 A
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same AWS designation
ProductClassRmKVAvailability
ELOX R 2209GedikE2209-17690–850 MPamin. 47 J (20 °C)To order · price and lead time in the quote