Kjellberg · Stainless steels
FINOX 4351 B — E 410 NiMo-15
covered electrode · stick electrodebasic coating
Choose the size
- Ø 3.25 × 450 mm · 5.3 kg≈ 5.3 kg
- Ø 4 × 450 mm · 5.3 kg≈ 5.3 kg
To order · price and lead time in the quote
We reply within 1 working day.
Field of application
High-efficiency basic electrode for welding matching soft martensitic chromium steels or cast steels. It is very well suited for cladding of stressed parts in power plant and hydropower plant construction – wear- and cavitation-resistant.
Base metals
1.4313 X 3 CrNiMo 13-41.4317 GX 4 CrNi 13-41.4413 X 3 CrNiMo 13-41.4414 GX 4 CrNiMo 13-4
| Positions | PA flat PB horizontal-vertical PC horizontal |
|---|---|
| Polarity | DC+ |
Classification and approvals
Classification
| AWS class | E 410 NiMo-15 |
|---|---|
| EN ISO class | E 13 4 B 52 |
| Material no. (W.-Nr.) | 1.4351 |
Composition and properties
Chemical composition of the weld metal
| C | 0.05 |
|---|---|
| Cr | 13.0 |
| Mn | 0.80 |
| Mo | 0.45 |
| Ni | 4.50 |
| Si | 0.50 |
Values in mass %.
Mechanical properties
after heat treatment: 600 °C / 2 h
| Yield strength (Rp0.2) | > 600 MPa |
|---|---|
| Tensile strength (Rm) | > 800 MPa |
| Elongation (A5) | > 15 % |
How to weld
Treatment and preparation
| Re-drying | 250–300 °C / 2 h |
|---|
Storage
In the original packaging, in dry, ventilated rooms: 5–30 °C, relative humidity < 60 %, up to 2 years.
| Moisture in the covering | More spatter and porosity: redry, above all when low hydrogen content is required. |
|---|
According to the Kjellberg 2019 catalogue
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 3.25 mm | 450 mm | 110–140 A |
| 4 mm | 450 mm | 130–170 A |
FERVEO guidance
By problem
Corrosion-resistant alloys