Gedik · Stainless steels
ELOX SG 308 L Si MIG — ER 308 LSi
solid wire
Choose the size
- Ø 0.8 mm · BS 300≈ 12.5 kg
- Ø 1 mm · BS 300≈ 15 kg
- Ø 1.2 mm · BS 300≈ 15 kg
- Ø 1.6 mm · BS 300≈ 15 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 135 · η 0.92–0.98
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
4.65–6.71 kg
of ELOX SG 308 L Si MIG for 10 m of weld
1 pack of 12.5 kg
Calculated with: η 0.92–0.98: typical value for process 135 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Which filler joins two different metals?With this product's data: 308L
With reservationsFN 1.6 (WRC-1992)
- The weld sits close to the martensite boundary: keep the dilution under control.
- Ferrite below 3 FN: risk of hot cracking (API RP 582, TWI).
Maximum dilution with this filler: 11.5 %
Calculated with: filler 308L — this product · dilution 20 % typical of 135, equal shares of each metal
See the full calculation →Field of application
- MIG welding of 13% Cr ferritic stainless steels, high-carbon steels of type 304 or stabilized steels of type 347, or steels of similar types, used in industries of drug, cellulose, paper, and food (production)
- Ar+%2.5 O2 or Ar+%2.5 CO2 mixed gas is used as shielding gas
- Maintenance of ductile behavior at temperature values down to -196°C.
- Maintenance of resistance to intergranular corrosion at temperatures up to 350°C
Base metals
X2 CrNi 19 11X5CrNi 18 10X6 CrNiTi 18 10X6 CrNiNb 18 10X2 CrNiN 18 10X10 CrNiNb 18 1O
AISI & ASTM:
304304L304LN321347A320Gr.B8CA320Gr.B8D
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up PG vertical-down |
|---|---|
| Polarity | DC+ |
| Shielding gas | Ar + 2.5% O2, Ar + 2.5% CO2 |
Classification and approvals
Classification
| AWS class | ER 308 LSi |
|---|---|
| EN ISO class | G 19 9 L Si |
Approvals
- CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the wire
| C | 0.02 |
|---|---|
| Cr | 20.4 |
| Mn | 1.70 |
| Ni | 10.2 |
| Si | 0.80 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | min. 350 MPa |
|---|---|
| Tensile strength (Rm) | 520–660 MPa |
| Elongation (A5) | min. 35 % |
| Impact energy (KV) | min. 63 J (20 °C) |
| Service temperature | −196–350 °C |
How to weld
Process
| Shielding | Requires shielding gas |
|---|
FERVEO guidance
By problem
Corrosion-resistant alloys
Alternatives in the catalogue
Same class
same EN ISO designation
| Product | Class | Rm | KV | Availability |
|---|---|---|---|---|
| DT-1.4316 MIGDratec | G 19 9 L Si | 590 MPa | 80 J | To order · price and lead time in the quote |