ELOX RS 308 — E308-26
covered electrode · stick electroderutile coating
Choose the size
- Ø 2.5 × 350 mm≈ 5 kg
- Ø 3.2 × 350 mm≈ 5 kg
- Ø 4 × 350 mm≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
7.02–11.21 kg
of ELOX RS 308 for 10 m of weld
3 packs of ≈ 5 kg
Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Field of application
- For joining and surfacing 18/8 Cr-Ni steels, high-strength quenched and tempered steels, stainless steels and non-alloy steels
- Metal recovery approx. 150 %
- Withstands high welding currents
- Redrying is required for at least 2 hours at 120 °C to 200 °C
Base metals
X2CrNi 1911X5CrNi 1911X5CrNi 18 8X12CrNi 17 7X12CrNi 18 8G-X10CrNi 18 8G-X12CrNi 18 8
AISI:
304 L304302301308
| Positions | PA flat PB horizontal-vertical PF vertical-up |
|---|---|
| Polarity | DC+/AC |
Classification and approvals
Classification
| AWS class | E308-26 |
|---|---|
| EN ISO class | E 19 9 R 53 |
Approvals
- TSE, CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.07 |
|---|---|
| Cr | 18.0 |
| Mn | 1.00 |
| Ni | 9.00 |
| Si | 0.80 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | min. 410 MPa |
|---|---|
| Tensile strength (Rm) | 570–710 MPa |
| Elongation (A5) | min. 30 % |
| Impact energy (KV) | min. 55 J (20 °C) |
How to weld
Treatment and preparation
| Re-drying | 120–200 °C / min. 2 h |
|---|
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 350 mm | 80–120 A |
| 3.2 mm | 350 mm | 110–160 A |
| 4 mm | 350 mm | 150–190 A |