ELOX R 318 — ~E318-16

covered electrode · stick electroderutile coating

Choose the size

  • Ø 2 × 250 mm
    ≈ 5 kg
  • Ø 2.5 × 250 mm
    ≈ 5 kg
  • Ø 3.2 × 300 mm
    ≈ 5 kg
  • Ø 3.2 × 350 mm
    ≈ 5 kg
  • Ø 4 × 350 mm
    ≈ 5 kg
To order · price and lead time in the quote

We reply within 1 working day.

How much filler metal do I need?With this product's data: 111 · η 0.55–0.65
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds

7.11–11.36 kg

of ELOX R 318 for 10 m of weld

3 packs of ≈ 5 kg

Calculated with: η 0.55–0.65: typical value for process 111 · preparation per EN ISO 9692-1 · EN ISO 5817 level C

See the full calculation →

Field of application

  • For welding tanks and pipes made of stabilised Cr-Ni-Mo alloy steels used in the food, chemical, textile and paint industries
  • The Nb-stabilised weld metal withstands temperatures up to +400 °C
  • Redrying is required for at least 2 hours at 120 °C to 200 °C

Base metals

EN:
X6CrNiMoTi 17 12 2X6CrNiMoNb 1 12 2X5CrNiMo 17 13 2G-XCrNiMo 18 10X10CrNiMoNb 18 12X5CrNiMo 17 13 3G-X10CrNiMo 18 10G-X10CrNiNb 18 10
AISI:
316Ti316Cb316L
PositionsPA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up
PolarityDC+/AC

Classification and approvals

Classification

AWS class~E318-16
EN ISO classE 19 12 3 Nb R 32

Approvals

  • TSE, CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order

Composition and properties

Chemical composition of the weld metal

C0.04
Cr19.4
Mn0.80
Mo2.80
Nbpresent
Ni11.0
Si0.80
Values in mass %.

Mechanical properties

Yield strength (Rp0.2)min. 390 MPa
Tensile strength (Rm)580–750 MPa
Elongation (A5)min. 30 %
Impact energy (KV)min. 47 J (20 °C)
Service temperaturemax. 400 °C

How to weld

Treatment and preparation

Re-drying120–200 °C / min. 2 h

Welding parameters by diameter

ØLengthCurrent
2 mm250 mm40–60 A
2.5 mm250 mm50–90 A
3.2 mm300 mm80–120 A
3.2 mm350 mm80–120 A
4 mm350 mm110–160 A
FERVEO guidance