Gedik · Stainless steels
ELOX R 317 L — E317L-16
covered electrode · stick electroderutile coating
Choose the size
- Ø 2.5 × 250 mm≈ 5 kg
- Ø 3.2 × 350 mm≈ 5 kg
- Ø 4 × 350 mm≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
Field of application
- Reduces the risk of intergranular carbide precipitation and so increases resistance to intergranular corrosion without stabilising elements such as niobium or titanium
- Electrode with an alloyed core wire and a rutile-basic covering for corrosion-resisting CrNi steels with increased Mo content
- Redrying is required for at least 2 hours at 120 °C to 200 °C
Base metals
EN:
X2CrNiMoN 17 13 3X2CrNiMoN 17 13 5X2CrNiMoN 18 18 3X2CrNiMoN 18 13X4CrNiMoN 19 16 5X4CrNiMoN 22 15X2CrNiMo 18 14 3X2CrNiMo 18 16 4X10CrNiMoTi 18 12
AISI & UNS:
316L316Cb317S31726
| Positions | PA flat PB horizontal-vertical PC horizontal PD horizontal-overhead PE overhead PF vertical-up |
|---|---|
| Polarity | DC+/AC |
Classification and approvals
Classification
| AWS class | E317L-16 |
|---|---|
| EN ISO class | E Z 19 13 4 L R 12 |
Approvals
- TSE, CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | < 0.04 |
|---|---|
| Cr | 18.7 |
| Mn | 0.90 |
| Mo | 3.20 |
| Ni | 12.5 |
| Si | 0.80 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | min. 400 MPa |
|---|---|
| Tensile strength (Rm) | 570–700 MPa |
| Elongation (A5) | min. 30 % |
| Impact energy (KV) | min. 47 J (20 °C) |
How to weld
Treatment and preparation
| Re-drying | 120–200 °C / min. 2 h |
|---|
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 250 mm | 50–90 A |
| 3.2 mm | 350 mm | 80–120 A |
| 4 mm | 350 mm | 110–160 A |
FERVEO guidance
By problem
Corrosion-resistant alloys