ELOX R 309 L — E309L-16
rev. 2 · 2026-11-21
page 1 / 2
- For similar austenitic stainless steels and dissimilar metals; buffer layers on non-alloy and low-alloy steels before build-up or surfacing with any stainless electrode; joining corrosion-resistant stainless steel to non-alloy or low-alloy steels; clad steels
- Good crack resistance on difficult-to-weld steels
- The weld metal has a high ferrite content
- Redrying is required for at least 2 hours at 120 °C to 200 °C
TSE, CE, BV, ABS, SEPRO, RCB, DNV-GL
Validity is confirmed with the order
High-strength unalloyed and heat-treatable steels · ferritic Cr and austenitic CrNi steels · austenitic Mn steels · Unalloyed tempered steels · tool steels · hard manganese steels · ferritic chromium steels · austenitic nickel-chromium steels · hard-to-weld steels
Typical values, not guaranteed: this document is not a declaration of performance and does not replace the manufacturer's official documentation or the applicable WPS.
Prepared by FERVEO from the Gedik 2023 catalogue