Gedik · Cast iron
ELNIKEL-NC — ENi-CI
covered electrode · stick electrode
Choose the size
- Ø 2.5 × 300 mm≈ 5 kg
- Ø 3.2 × 300 mm≈ 5 kg
- Ø 4 × 400 mm≈ 5 kg
To order · price and lead time in the quote
We reply within 1 working day.
Field of application
- Non-conductive, basic-graphite-coated nickel stick electrode
- Repair welding of problematic cast iron parts of irregular shapes
- Joint welding of cast iron parts, and cast iron parts to steel parts
- Pre-heating to 200 °C is recommended for thick-walled components
- Welding in short runs, and peening are required
| Positions | PA flat PB horizontal-vertical PF vertical-up |
|---|---|
| Polarity | DC+ |
Classification and approvals
Classification
| AWS class | ENi-CI |
|---|---|
| EN ISO class | E C Ni-CI 1 |
Approvals
- CE, SEPRO, TSE
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.50 |
|---|---|
| Ni | min. 96.0 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | 200 MPa |
|---|---|
| Tensile strength (Rm) | 250 MPa |
| Elongation (A5) | 3 % |
Hardness
- approx. 170 HB
How to weld
Treatment and preparation
| Pre-heating | 200 °C, for thick-walled components |
|---|
Welding parameters by diameter
| Ø | Length | Current |
|---|---|---|
| 2.5 mm | 300 mm | 70–100 A |
| 3.2 mm | 300 mm | 90–110 A |
| 4 mm | 400 mm | 110–130 A |
FERVEO guidance
By problem
Cast iron
Alternatives in the catalogue
Same class
same EN ISO designation · same AWS designation
| Product | Class | Rm | Availability |
|---|---|---|---|
| ELNIKELGedik | E C Ni-CI 1 | 250 MPa | To order · price and lead time in the quote |
| ELNIKEL - HDGedik | ENi-CI | 250 MPa | To order · price and lead time in the quote |
| FICAST NIKjellberg | ENi-CI | > 400 MPa | To order · price and lead time in the quote |
| Ni - CASTGedik | E C Ni-CI 1 | 240–300 MPa | To order · price and lead time in the quote |
| Ni-CAST BFNCGedik | E C Ni-CI 1 | 335 MPa | To order · price and lead time in the quote |