Gedik · Submerged arc fluxes
ELIFLUX BFPV — F7A2-EM12/F7A2-EM12K
flux
Choose the size
- kraft paper bag≈ 25 kg
To order · price and lead time in the quote
We reply within 1 working day.
Field of application
- GeKa ELIFLUX BFPV, high basic, is agglomerated fluoride basic flux for submerged arc welding.
- It features high impact toughness and low hydrogen content
- It is suitable for double wire welding and narrow gap welding of thick steel plates, pressure vessels
- Flux should be re-dried before use for 2 hours at 300°C - 350°C
Classification and approvals
Classification
| AWS class | F7A2-EM12/F7A2-EM12K |
|---|---|
| EN ISO class | SA FB 1 66 AC H5 |
Approvals
- SEPRO, CE
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
with wire S2 — F7A2-EM12
| C | 0.06 |
|---|---|
| Mn | 1.20 |
| Si | 0.35 |
with wire S2 Si — F7A2-EM12K
| C | 0.07 |
|---|---|
| Mn | 1.25 |
| Si | 0.40 |
with wire S2 Mo — F8A4-EA2-A2
| C | 0.07 |
|---|---|
| Mn | 1.30 |
| Mo | 0.50 |
| Si | 0.40 |
with wire S3NiCrMo2.5 — F11A8-EM4(mod.)-M4
| C | 0.06 |
|---|---|
| Cr | 0.40 |
| Mn | 1.75 |
| Mo | 0.50 |
| Ni | 2.10 |
| Si | 0.40 |
with wire S3 Mo
| C | 0.05 |
|---|---|
| Mn | 1.75 |
| Mo | 0.50 |
| Si | 0.30 |
Values in mass %.
Mechanical properties
with wire S2 — F7A2-EM12
| Yield strength (Rp0.2) | 430 MPa |
|---|---|
| Tensile strength (Rm) | 520 MPa |
| Elongation (A5) | 29 % |
| Impact energy (KV) | 60 J (−30 °C) |
with wire S2 Si — F7A2-EM12K
| Yield strength (Rp0.2) | 440 MPa |
|---|---|
| Tensile strength (Rm) | 515 MPa |
| Elongation (A5) | 30 % |
| Impact energy (KV) | 65 J (−30 °C) |
with wire S2 Mo — F8A4-EA2-A2
| Yield strength (Rp0.2) | 490 MPa |
|---|---|
| Tensile strength (Rm) | 595 MPa |
| Elongation (A5) | 26 % |
| Impact energy (KV) | 60 J (−40 °C) |
with wire S3Si — F8A5-EA4-A3
| Yield strength (Rp0.2) | 500 MPa |
|---|---|
| Tensile strength (Rm) | 588 MPa |
| Elongation (A5) | 27 % |
| Impact energy (KV) | 100 J (−40 °C) · 80 J (−50 °C) |
with wire S3NiCrMo2.5 — F11A8-EM4(mod.)-M4
| Yield strength (Rp0.2) | 700 MPa |
|---|---|
| Tensile strength (Rm) | 775 MPa |
| Elongation (A5) | 23 % |
| Impact energy (KV) | 55 J (−40 °C) · 45 J (−50 °C) · min. 27 J (−60 °C) |
How to weld
Treatment and preparation
| Re-drying | 300–350 °C / 2 h |
|---|
FERVEO guidance
Alternatives in the catalogue
Same class
same AWS designation
| Product | Class | Availability |
|---|---|---|
| ELIFLUX BFPPGedik | F7A2-EM12/F7A2-EM12K | To order · price and lead time in the quote |