Gedik · Submerged arc fluxes
ELIFLUX BFF — F7A4-EM12/F7A4-EM12K/ F7A4-EH12K
flux
Choose the size
- kraft paper bag≈ 25 kg
To order · price and lead time in the quote
We reply within 1 working day.
Field of application
- This is fluoride-basic agglomerated flux
- This flux is suitable for welding high strength low alloy steels
- Preferable to use with wire electrodes having higher manganese level
- Recommended for multi-pass welding, in particular when there are high toughness requirement
- Process requirement of re-drying at 300°C - 350°C for 2 hours
Classification and approvals
Classification
| AWS class | F7A4-EM12/F7A4-EM12K/ F7A4-EH12K |
|---|---|
| EN ISO class | SA FB 1 65 DC H5 |
Approvals
- CE, SEPRO
- S2Si x ELIFLUX BFF: BV, ABS, CE
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
with wire S2 — F7A4-EM12
| C | 0.05 |
|---|---|
| Mn | 1.00 |
| Si | 0.20 |
with wire S2 Si — F7A4-EM12K
| C | 0.06 |
|---|---|
| Mn | 1.10 |
| Si | 0.30 |
with wire S2 Mo — F8A4-EA2-A2
| C | 0.07 |
|---|---|
| Mn | 1.15 |
| Mo | 0.45 |
| Si | 0.25 |
with wire S3 Si — F7A4-EH12K
| C | 0.10 |
|---|---|
| Mn | 1.70 |
| Si | 0.60 |
with wire S3 NiMo1 — F9A4-EF3(mod)-F3
| C | 0.09 |
|---|---|
| Mn | 1.65 |
| Mo | 0.55 |
| Ni | 0.90 |
| Si | 0.25 |
with wire S3NiCrMo2.5 — F11A8-EM4(mod.)-M4
| C | 0.06 |
|---|---|
| Cr | 0.50 |
| Mn | 1.50 |
| Mo | 0.50 |
| Ni | 2.20 |
| Si | 0.30 |
Values in mass %.
Mechanical properties
with wire S2 — F7A4-EM12
| Yield strength (Rp0.2) | 410 MPa |
|---|---|
| Tensile strength (Rm) | 520 MPa |
| Elongation (A5) | 24 % |
| Impact energy (KV) | 70 J (−30 °C) · 60 J (−40 °C) |
with wire S2 Si — F7A4-EM12K
| Yield strength (Rp0.2) | 450 MPa |
|---|---|
| Tensile strength (Rm) | 540 MPa |
| Elongation (A5) | 23 % |
| Impact energy (KV) | 65 J (−40 °C) |
with wire S2 Mo — F8A4-EA2-A2
| Yield strength (Rp0.2) | 480 MPa |
|---|---|
| Tensile strength (Rm) | 570 MPa |
| Elongation (A5) | 27 % |
| Impact energy (KV) | 70 J (−40 °C) |
with wire S3 Si — F7A4-EH12K
| Yield strength (Rp0.2) | 490 MPa |
|---|---|
| Tensile strength (Rm) | 580 MPa |
| Elongation (A5) | 26 % |
| Impact energy (KV) | 60 J (−40 °C) |
with wire S3 NiMo1 — F9A4-EF3(mod)-F3
| Yield strength (Rp0.2) | 580 MPa |
|---|---|
| Tensile strength (Rm) | 650 MPa |
| Elongation (A5) | 21 % |
| Impact energy (KV) | 100 J (−20 °C) · 60 J (−40 °C) |
with wire S3NiCrMo2.5 — F11A8-EM4(mod.)-M4
| Yield strength (Rp0.2) | 740 MPa |
|---|---|
| Tensile strength (Rm) | 850 MPa |
| Elongation (A5) | 20 % |
| Impact energy (KV) | 90 J (−20 °C) · 85 J (−40 °C) · min. 27 J (−60 °C) |
How to weld
Treatment and preparation
| Re-drying | 300–350 °C / 2 h |
|---|
FERVEO guidance
Used together with