Gedik · Carbon steels
ELCOR MR 70 FCW — E 70 T-9 C J H 8
flux-cored wire (FCW)
Choose the size
- Ø 1.2 mm · BS 300≈ 15 kg
To order · price and lead time in the quote
We reply within 1 working day.
How much filler metal do I need?With this product's data: 136 · η 0.80–0.90
Thickness of the plates to be joinedref. 1.3: 3 < t ≤ 10
Sum of all identical welds
5.03–7.66 kg
of ELCOR MR 70 FCW for 10 m of weld
1 pack of 15 kg
Calculated with: η 0.80–0.90: typical value for process 136 · preparation per EN ISO 9692-1 · EN ISO 5817 level C
See the full calculation →Do I need to preheat?With this product's data: H10
Thickness of the thickest part in the jointmethod B: d from 10 to 90 mm
135 °C
Minimum preheat and minimum interpass temperature
EN 1011-2, annex C, method B · rounded up to 5 °C
✓ Within the range of method B.
Calculated with: HD 10 ml/100 g from this product's class H10 · 136 — gas-shielded flux-cored: 26 V, 220 A, 30 cm/min
See the full calculation →Field of application
- Metal-rutile cored wire
- High deposition rate and therefore deeper penetration
- Suitable for fillet welds in the flat (PA) and horizontal (PB) positions
- Excellent impact toughness at low temperatures
- Shielding gas: CO2
| Positions | PA flat PB horizontal-vertical |
|---|---|
| Polarity | DC+ |
| Shielding gas | CO2 |
Classification and approvals
Classification
| AWS class | E 70 T-9 C J H 8 |
|---|---|
| EN ISO class | T 42 4 R C3 H10 |
Approvals
- CE, SEPRO
According to the Gedik 2023 catalogue; validity is confirmed with the order
Composition and properties
Chemical composition of the weld metal
| C | 0.04 |
|---|---|
| Mn | 1.40 |
| Si | 0.70 |
Values in mass %.
Mechanical properties
| Yield strength (Rp0.2) | min. 420 MPa |
|---|---|
| Tensile strength (Rm) | 500–640 MPa |
| Elongation (A5) | min. 22 % |
| Impact energy (KV) | min. 47 J (−40 °C) |
How to weld
Process
| Shielding | Requires shielding gas |
|---|
FERVEO guidance
By problem
Structural steels